1-20 of 28 Search Results for

JESSOP 2-B

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1955) 4 (5): TS-33.
Published: 01 May 1955
... JESSOP 2-B is a general purpose hot work die steel having great resistance to abrasion. It is supplied in three grades. namely 2-B (L.C.), 2-B (M.C.) and 2-B (H.C.). These are classed as ASM Type IV F1, Type IV F3 and Type IV F2 respectively. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1988) 37 (10): Ni-363.
Published: 01 October 1988
... JESSOP JS Alloy B-2 is a nickel-molybdenum alloy with outstanding corrosion resistance in the as-welded condition. It can be used up to 1000 F and, with proper atmospheric protection, above 1500 F. In the range 1000-1500 F the alloy exhibits reduced ductility and use in that temperature range...
Journal Articles
Alloy Digest (1983) 32 (12): TS-419.
Published: 01 December 1983
... As quenched - 1000 5 5:: 1100 2+2 1150 2+2 1200 2+2 Rockwell C Hardness 48-50 50-52 47-49 46-48 43-45 32-34 Heal Treatment: Annealing: Heat Jessop Dica B Vanadium tool steel slowly and uniformly to 1625 F, soak well to equalize the temperature and then cool slowly (400 F maximum per hour) in the furnace...
Journal Articles
Alloy Digest (1986) 35 (8): Ni-337.
Published: 01 August 1986
... treatment at 2 I 50° F followed by rapid 3 I6 to 3,4 in. Over 3,4 in. 90000 85000 35000 30000 35 30 cooling ensures maximum ductility. corrosion resistance and machinability of Jessop Alloy G. DOI: 10.31399/asm.ad.ni0337 Copyright © ASM International® 1996 Machinability: Machinability rating of Jessop Alloy...
Journal Articles
Alloy Digest (1983) 32 (4): Ni-285.
Published: 01 April 1983
...-reactor components oxidation resistance physical properties tensile properties workability UNS N06625 All JESSOP JS625 Flllng Code: Ni-285 Or Nickel Alloy APRIL 1983 DIGEST - DATA ON WORLD WIDE MeTAls AND AUOYS @ Copyright 1980, Engineering Publications. Inc. Ail rights reserved. Published b t MN...
Journal Articles
Alloy Digest (1983) 32 (10): Ni-293.
Published: 01 October 1983
... Temperature Modulus (Dynamic) F (Tension), psi 80 28.3 x 106 500 26.4 1000 23.8 1200 22.7 1350 21.7 I500 20.3 1600 19.4 1700 18.3 1800 17.3 0.294 8. I4 25OG 2550 7.8 x IO+ 83 x lo-6 85x lo+ 87x IO-b 8.8 x IO 9.1x lo-6 9.5x IO+ 9.7 x IO-b See Table I I. 005 -320 See Table 2 Table 3 - ROOM-TEMPERATURE...
Journal Articles
Alloy Digest (1960) 9 (6): SA-99.
Published: 01 June 1960
... heat treatability JESSOP no. 200 joinability machinability magnetic permeability physical properties tensile properties workability JESSOP No. 200 Filing Code: SA-99 Steel-Alloy B JUNE 1960 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS P&isbd by Engineering Alloys Digear, Inc. upper bhmhir...
Journal Articles
Alloy Digest (1988) 37 (4): Ni-330.
Published: 01 April 1988
... 1996 Heat Treatment: Jessop JS Alloy 276 is used in the annealed (solution- treated) condition. It is annealed by heating to the 2050-2lOO F range and quenched in water or rapidly cooled by other means. The mechanical properties in the annealed condition are given in Tables I and 2. Machining...
Journal Articles
Alloy Digest (1984) 33 (4): TS-422.
Published: 01 April 1984
... Steel APRIL 1984 - DATA ON WORLD WIDE METALS AND ALLOYS Published b> @ &pyripht 1980. bIQiMi?rhQ PubliCOtionS. k. Ait rights rCSWw?d. ISSN : 002-614X Alloy Digest. Inc. Post Office Box 823 Upper Montclair, New Jersey JESSOP* SUPERSHOCK 7 (Air-Hardening Shock Steel: AISI Type S7) JEfjSOp SUPERSHOCK 7...
Journal Articles
Alloy Digest (1989) 38 (7): SS-509.
Published: 01 July 1989
... Elongation (2 in % (min) 40 40 Reduction in area, % (min) 50 50 Hardness, Brinell (max) 217 217 Rockwell B (max) 95 95 Heat Treatment: Workability: JESSOP Types 316L and 316LM are austenitic stainless steels and so are not hardenable by heat treatment. They may be annealed by heating to and rapidly cooling...
Journal Articles
Alloy Digest (1982) 31 (3): SS-404.
Published: 01 March 1982
... Remainder PROPERTIES Table 1 - MECHANICAL PROPERTIES (Annealed condition) Tensile strength, psi, min Yield strength (0.2% offset), psi, min Elongation (2 in %, min Reduction of area, %, min Brinell hardness, max Rockwell B hardness, max 71000 31000 35 40 192 90 Heat Treatment: Solution Annealing: Heat...
Journal Articles
Alloy Digest (1984) 33 (6): SS-448.
Published: 01 June 1984
... 19.2 Table 2 - ROOM-TEMPERATURE MECHANICAL PROPERTIES (Minimum values) 0.287 7.94 2475-2525 7.9 x 10-b 1.014 -175 See Table I Property JS800 JSSOOH Tensile strength, psi 65000 75000 Yield strength (0.20/, offset), psi 25000 30000 Elongation (2 in % 30 30 DOI: 10.31399/asm.ad.ss0448 Copyright © ASM...
Journal Articles
Alloy Digest (1987) 36 (5): Ni-348.
Published: 01 May 1987
... Over 314 Tensile strength, psi, min. 90000 85000 Yield strength (0.2% offset), psi, min. 35000 30000 Elongation (2 in %, min. 45 35 DOI: 10.31399/asm.ad.ni0348 Copyright © ASM International® 1996 Heat Treatment: JESSOP JS alloy G-3 is generally supplied in the solution heat-treated condition...
Journal Articles
Alloy Digest (1987) 36 (8): SS-488.
Published: 01 August 1987
... gravity 7.90 Melting range, F 2500-2550 Specific heat, Btu/lbF (32-212 F) 0.12 Thermal coef. expansion: OF (32-2 12 F) 8.9 x 10-b Thermal conductivity. Btu/ftr/ft/ hr/ OF (At 212OF) 8.9 Electrical resistivity, microhm-cm (At 68 F) 73 Modulus of elasticity, psi 28 x 106 Magnetic characteristics...
Journal Articles
Alloy Digest (1983) 32 (6): Ni-287.
Published: 01 June 1983
.... Details for pickling are available from the manufacturer. Specification Equivalents: ASTM B 168. UNS No. N06600. Generai Characteristics: As stated in the introduction, Jessop JS600 is a nickel- chromium-iron alloy for use in environments requiring resistance to heat and corrosion. The high nickel content...
Journal Articles
Alloy Digest (1984) 33 (2): SS-440.
Published: 01 February 1984
... various heat-treated conditions (Figure I). Jessop JS I7Cr-7Ni machines like martensitic stainless steels of equal hardness. Workability: Jessop JS I7Cr-7NI has good hot-uorking characteristics. In Condition A (mill annealed) it can be cold worked readily b> any of Ihe conventional processes. Wefding...
Journal Articles
Alloy Digest (1983) 32 (8): Ni-289.
Published: 01 August 1983
... (2 in %a min 35 30 DOI: 10.31399/asm.ad.ni0289 Copyright © ASM International® 1996 Heat Treatment: Annealing (Solution Treatment): Heat hot-worked or cold-worked Jessop JS Alloy G to 205&21500F, hold at temperature long enough for solution of alloy constituents (about 15 minutes), and quench...
Journal Articles
Alloy Digest (1964) 13 (5): SA-164.
Published: 01 May 1964
... followed by air cooling or annealing at 16OOoF followed by slow (500F max. per hour) cooling to 1lOOoF is essential. Specification Equivalents: Brirish En.40C British DTD55 1 General Characteri sties: Jessop Saville H.2 exhibits high tensile srrengch and high skin hardness after nitriding. Maximum recom...
Journal Articles
Alloy Digest (1981) 30 (8): TS-385.
Published: 01 August 1981
... many applications include blanking dies, coining, cold shears and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-385. Producer or source: Jessop Steel...
Journal Articles
Alloy Digest (1969) 18 (3): TS-215.
Published: 01 March 1969
... toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-215. Producer or source: Jessop Steel Company. Producer or Source: Jessop Steel Company Copyright © ASM International® 1996 1996 ASM International abrasive wear resistance brick mold...