1-5 of 5 Search Results for

JALLOY 1

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1957) 6 (11): SA-3.
Published: 01 November 1957
... JALLOY 1 is a fine grain, high quality steel for jobs where formability is an important consideration or where use of a low carbon steel with good mechanical properties before or after heat treatment are desired. This datasheet provides information on composition, hardness, and tensile properties...
Journal Articles
Alloy Digest (1963) 12 (4): SA-144.
Published: 01 April 1963
... by the grade designation. Where guaranteed mechanical properties are required, acceptable limits can be negotiated. Table 2 - ELEVATED TEMPERATURE PROPERTIES - SlOO (1 plate of Jalloy-S-100) Test Tensile Temperature Strength OF DSi 70 115000 400 110000 600 111250 800 96000 900 89500 1000 77600 Yield Strength...
Journal Articles
Alloy Digest (1963) 12 (9): SA-153.
Published: 01 September 1963
..., lbjcu.in. Thermal coef. expansion,;oF x 10-6 Modulus of elasticity, psi x 106 0.283 7.25 30 PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES Tensile Yield Reduction Strength Strength Elongation of Area Brine11 Grade psi psi (0.2%) y. in 2 % Hardness J alloy-AR-360 155000 140000 15.0 55.0 340-380 Jalloy...
Journal Articles
Alloy Digest (1958) 7 (1): SA-65.
Published: 01 January 1958
... JALLOY 3 is a general purpose steel which is capable of being heat treated to excellent mechanical properties. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on heat treating, machining, and joining...
Journal Articles
Alloy Digest (1963) 12 (1): SA-32.
Published: 01 January 1963
... JALLOY 7 is a manganese-molybdenum oil-hardening steel applicable where high hardness with good ductility or wear resistance is desirable. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on heat...