Skip Nav Destination
Close Modal
Search Results for
Ispat Inland MartINsite
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Ispat Inland MartINsite
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (2): CS-62.
Published: 01 February 2003
... Ispat Inland MartINsite is a low-carbon cold-rolled ultrahigh-strength steel available in four grades with minimum tensile strengths of 900 MPa (130 ksi) (M-130), 1100 MPa (160 ksi) (M-160), 1310 MPa (190 ksi) (M-190), and 1520 MPa (220 psi) (M-220). This steel can be used where high strength...
Abstract
View article
PDF
Ispat Inland MartINsite is a low-carbon cold-rolled ultrahigh-strength steel available in four grades with minimum tensile strengths of 900 MPa (130 ksi) (M-130), 1100 MPa (160 ksi) (M-160), 1310 MPa (190 ksi) (M-190), and 1520 MPa (220 psi) (M-220). This steel can be used where high strength and/or lightweight are required and can substitute for high-carbon alloy steels, spring steels, and some nonferrous alloys at significant savings in cost. Electrosite is an electrogalvanized form of M-190. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on wear resistance as well as heat treating and surface treatment. Filing Code: CS-62. Producer or source: Ispat Inland Inc. Originally published as Inland MartINsite, October 1976, revised February 2003.