1-3 of 3 Search Results for

Industeel D2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2020) 69 (4): TS-791.
Published: 01 April 2020
... Industeel D2 is an air-hardening, high-carbon (1.5%), high-chromium (12%), alloy cold-work tool steel that also contains molybdenum and vanadium. It is specifically designed to provide high abrasive wear resistance and high hardenability. This grade can be used for cutting and deformation tools...
Journal Articles
Alloy Digest (2020) 69 (6): TS-795.
Published: 01 June 2020
... Industeel Tenasteel is a high-carbon, chromium-molybdenum-vanadium, alloy cold-work tool steel that is specially designed to replace Type D2 and X153CrMoV12 (1.2379) cold work tool steels in applications requiring high wear resistance and very good toughness. This datasheet provides information...
Journal Articles
Alloy Digest (2014) 63 (5): SA-700.
Published: 01 May 2014
... on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-700. Producer or source: Industeel USA, LLC. Producer or Source: Industeel USA, LLC Copyright ┬ę ASM International┬« 2014...