1-11 of 11

Search Results for Inconel alloy 751

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1966) 15 (8): Ni-116.
Published: 01 August 1966
... INCONEL alloy 751 is a high-strength, high-temperature nickel-chromium alloy. It is essentially the same as INCONEL alloy X-750, except that its slightly modified composition imparts increased rupture properties at 1600 F. It is used for diesel engine exhaust valves. This datasheet provides...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1229.
Published: 01 October 2015
... and can be welded similar to normal austenitic stainless steel using Inconel 82, Inconel 625, and Hastelloy C-276 welding materials Product Forms Available: This alloy is available in a wide range of plate, sheet, and strip (see Fig. 3). This material requires special consultation for sheet thicknesses...
Journal Articles
Alloy Digest (2021) 70 (10): Ni-776.
Published: 01 October 2021
... 980 °C (1800 °F). Hot work- ATI ing temperatures between 650 and 870 °C (1200 and 1600 ISO 683-15:1992 UNS N07751 °F) should be avoided. SAE J775:2018 Inconel 751 Special Metals Corporation VDM 751 (Nicrofer 7016 TiAl) Cold Forming VDM Metals GmbH ATI X-751 is cold formed in the solution annealed...
Journal Articles
Alloy Digest (2015) 64 (12): SS-1234.
Published: 01 December 2015
.... Excellent resistance to acids and stress corrosion cracking by chlorides; is better than SUS316. Higher mechanical strength than SUS316. Copyright © 2015, ASM International®. All rights reserved. Good weldability, as well as current austenitic stainless steel, using welding consumables Inconel 625...
Journal Articles
Alloy Digest (1975) 24 (1): Ni-213.
Published: 01 January 1975
... Crucible test sultidation, 55 CaS04, 30 BaS04, IO Na2S04.5 C 1700/l 0.80 0.82 0.84 Crucible test sultidation. 10 NaCl, 90 Na2SO4 I7001 I 0.014 0.034 0.055 l SAE EV 8 (214N) is a standard valve alloy containing. in I: 0.53 C. 9.00 Mn. 0.15 Si, 21 .OO Cr. 3.75 Ni. 0.42N. 0.07 S, balance Fe. **INCONEL 751...
Journal Articles
Alloy Digest (1988) 37 (6): Ni-109.
Published: 01 June 1988
... as for INCONEL* Alloy 600. Use well powered equipment with good rigidity. The work hardening rate of the alloy is somewhat less than that of austenitic stainless steels but it is still relatively high. Weldability: INCOLOY Alloy 825 has good weldability by all conventional processes. INCOLOY Welding Electrode...
Journal Articles
Alloy Digest (1970) 19 (11): Ni-159.
Published: 01 November 1970
... INCONEL Alloy 706 is a precipitation-hardenable, nickel-iron-chromium alloy with high strength at temperatures to 1300 F and with good resistance to oxidation and corrosion over a broad range of temperatures and environments. Its characteristics are similar to those of INCONEL Alloy 718, except...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... Inconel alloy 22 is an advanced corrosion-resistant alloy with exceptional resistance to aqueous and pitting corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1989) 38 (2): Ni-368.
Published: 01 February 1989
... is a precipitation-hardenable, nickel-iron-chromium alloy with high strength at temperatures to 1200°F and with good rtxiaan~ to oxidation and corrosion over a broad range of temperatures and environments. *Inconel is a registered trademark of the Into family of alloys. Composition: Nickel Chromium Columbium...
Journal Articles
Alloy Digest (2006) 55 (5): SS-962.
Published: 01 May 2006
...) in an Acidified 6% Ferric Chloride Solution CCT CPT Alloy °C °F °C °F Inconel 625 30 35 86 95 >85 >185 Incoloy 25-6Mo 30 35 86 95 70 158 Alloy 904L 12.5 54 37.5 99 AISI 316L <0 <32 20 68 AISI 317LM 20 68 52.5 126 AISI 304 <0 <32 15 59 ...
Journal Articles
Alloy Digest (1983) 32 (12): Ni-295.
Published: 01 December 1983
... worked by the conventional methods used for nickel alloys. JoinabUlfy: HUNTINGTON alloy G has good weldability and needs no post- weld heat treatment to restore corrosion resistance Recommended welding products for alloy G are lNCONEL@ Welding Electrode I I2 for shielded-metal-arc welding and INCONEL...