Alloy Digest (1970) 19 (11): Ni-159.
Published: 01 November 1970
... INCONEL Alloy 706 is a precipitation-hardenable, nickel-iron-chromium alloy with high strength at temperatures to 1300 F and with good resistance to oxidation and corrosion over a broad range of temperatures and environments. Its characteristics are similar to those of INCONEL Alloy 718, except...
Journal Articles
Alloy Digest (1989) 38 (2): Ni-368.
Published: 01 February 1989
... is a precipitation-hardenable, nickel-iron-chromium alloy with high strength at temperatures to 1200°F and with good rtxiaan~ to oxidation and corrosion over a broad range of temperatures and environments. *Inconel is a registered trademark of the Into family of alloys. Composition: Nickel Chromium Columbium...
Journal Articles
Alloy Digest (1963) 12 (7): Cu-130.
Published: 01 July 1963
... REVERE NO. 770 is an 18% nickel silver alloy having high malleability, high modulus of elasticity and high resistance to corrosion. It is a spring stock alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue...
Journal Articles
Alloy Digest (1986) 35 (6): Ni-333.
Published: 01 June 1986
... INCONEL Filler Metal 718 is used for gas-tungsten-arc welding of INCONEL alloys 718, 706 and X-750. The weld metal is age hardenable and its mechanical properties are comparable to those of the base metals. This datasheet provides information on composition and tensile properties. It also includes...
Journal Articles
Alloy Digest (2013) 62 (1): Ni-706.
Published: 01 January 2013
... Products Corporation Copyright © ASM International® 2013 2013 ASM International chemical composition ductility heat treatability Inconel Filler Metal 52MSS joinability tensile properties workability UNS N06055 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®...