1-1 of 1 Search Results for

Inconel alloy 050

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2005) 54 (12): Ni-629.
Published: 01 December 2005
... Inconel alloy 050 is an improved corrosion-resistant alloy in tubular form for down hole service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing...