Alloy Digest (2013) 62 (1): Ni-706.
Published: 01 January 2013
... Inconel Filler Metal 52MSS contains about 2.0–2.5 wt.% Nb and 3.0–4.0 wt% Mo, which have been shown to improve resistance to ductility dip cracking, and has reduced aluminum and titanium, which provide the ability to deposit very clean weld deposits without the floating oxide impurities of other...