Alloy Digest (1958) 7 (3): Ni-40.
Published: 01 March 1958
... INCONEL 702 is a nickel-base alloy having moderate strength with exceptional oxidation resistance at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion...
Journal Articles
Alloy Digest (1970) 19 (4): Ni-152.
Published: 01 April 1970
... cyclic oxidation. To emphasize the effectiveness of alloy 601 in such an environment, data are also included for three other materials with well demonstrated oxidation resistance - a 22 Cr-18.5 Fe-g.0 Mol.5 Co-O.6 W-Bal. Ni ailoy, 50 Ni-50 Cr alloy, and INCONEL alloy 702. Alloy 601 shows a significant...