Publisher: Journals Gateway
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
... INCONEL Alloy 690 is a wrought nickel-base alloy with excellent resistance to many corrosive aqueous media and high-temperature atmospheres. It also has high strength, good metallurgical stability, and favorable fabrication characteristics. It has excellent resistance to stress-corrosion cracking...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (7): Ni-288.
Published: 01 July 1983
... INCONEL Alloy MA 6000 is a nickel-base alloy produced by mechanical alloying. It is strengthened by both oxide dispersion strengthening and precipitation hardening for high creep and rupture properties at 2000 F (1095 C) as well as at 1400 F (760 C). The alloy's composition also gives it excellent...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (7): Ni-300.
Published: 01 July 1984
... INCONEL Welding Electrode 117 is a nickel-base alloy developed for welding a number of alloys. Its all-weld-metals strength and ductility are satisfactory for many uses. It is used for all-position shielded metal-are welding of INCONEL alloy 617. It is also recommended for the welding of a number...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (9): Ni-302.
Published: 01 September 1984
... INCONEL Filler Metal 617 is a nickel-base alloy suitable for welding a number of alloys. It is used for the gas tungsten-arc (TIG) and gas metal-arc (MIG) welding of INCONEL alloy 617. For extended service at temperatures above 1700 F (925 C), it is recommended for welding INCOLOY alloy 800H...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (4): Ni-313.
Published: 01 April 1985
... INCONEL Welding Electrode 112 is a nickel-base alloy that is used for welding INCONEL alloys 625 and 601 and INCOLOY alloy 800H. It is also used for surfacing steel and various corrosion-resistant alloys such as HUNTINGTON alloys G and 9041. It is useful for joining dissimilar metals involving...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (5): Ni-315.
Published: 01 May 1985
... INCONEL Filler Metal 92 is a nickel-base alloy that is used for gas-tungsten-arc and gas-metal-arc welding of austenitic and ferritic steels and nickel alloys. Applications include (1) Joining INCONEL and INCOLOY alloys to stainless steels, carbon steels and MONEL alloys, (2) Joining MONEL alloys...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (10): Ni-323.
Published: 01 October 1985
... IONCONEL Welding Electrode 132 is used for shielded-metal-arc welding of INCONEL alloys 600 and 601 and INCO alloy 330. Electrode 132 has good dissimilar-welding capability. Examples are joining INCONEL and INCOLOY alloys to carbon steels, stainless steels, nickel and MONEL alloys. It also is used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (11): Ni-325.
Published: 01 November 1985
... INCONEL Welding Electrode 182 is used for shielded-metal-arc welding of INCONEL alloys 600, 601 and 690. Dissimilar welds for which the electrode is used include INCONEL and INCOLOY alloys joined to carbon steels, stainless steels, nickel and MONEL alloys; MONEL alloys joined to carbon steels...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (12): Ni-327.
Published: 01 December 1985
... INCONEL Filler Metal 625 is used for gas-metal-arc and gas-tungsten-arc welding of INCONEL alloys 625 and 601 and INCOLOY alloy 800H. It is also used for surfacing of steel, for welding nickel steels, and for welding various corrosion-resistant alloys such as INCO Alloys G and 904L. It has high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (3): Ni-40.
Published: 01 March 1958
... INCONEL 702 is a nickel-base alloy having moderate strength with exceptional oxidation resistance at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (2): Ni-50.
Published: 01 February 1959
... INCONEL 713C is a nickel-chromium cast alloy which possesses outstanding rupture strength at 1700 F. combined with excellent resistance to thermal fatigue and good castability. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (3): Ni-56.
Published: 01 March 1960
... INCONEL 600 nickel-base alloy has better high temperature properties than Inconel alloy, particularly where rupture strength, creep and short-time tensile are necessary. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (6): Ni-58.
Published: 01 June 1960
... INCONEL W is a high strength, high temperature nickel-base alloy responding to an age-hardening heat treatment for maximum properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (11): Ni-471.
Published: 01 November 1994
... INCONEL alloy 718SPF is an age-hardenable austenitic material whose strength is largely dependent on the precipitation of a gamma prime phase following heat treatment. The base alloy, however, possesses two-essential characteristics for super-plastic forming; grain size stability over time...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (5): Ni-511.
Published: 01 May 1996
... Inconel alloy MA 758 is a further development of the well-established aerospace superalloy Inconel alloy MA 754 (Alloy Digest Ni-244, March 1990) with an increased chromium content for better resistance to high-temperature corrosives. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (4): Ni-152.
Published: 01 April 1970
... INCONEL Alloy 601 is a nickel-chromium solid-solution alloy with excellent high-temperature properties which make it attractive for many application in aerospace and process industries. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (11): Ni-159.
Published: 01 November 1970
... INCONEL Alloy 706 is a precipitation-hardenable, nickel-iron-chromium alloy with high strength at temperatures to 1300 F and with good resistance to oxidation and corrosion over a broad range of temperatures and environments. Its characteristics are similar to those of INCONEL Alloy 718, except...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (7): Ni-176.
Published: 01 July 1972
... INCONEL alloy 600 (formerly INCONEL, Alloy Digest Ni-9, March 1954) is a nickel-chromium-iron alloy with good resistance to corrosion and heat. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with a desirable combination of high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (9): Ni-179.
Published: 01 September 1972
... INCONEL Alloy 617 is a solid solution nickel-chromium-cobalt-molybdenum alloy having excellent high-temperature strength and oxidation resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (10): Ni-180.
Published: 01 October 1972
... INCONEL ALLOY 671 is a nickel-chromium alloy having excellent resistance to high-temperature corrosion. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance...