Alloy Digest (1970) 19 (7): SS-240.
Published: 01 July 1970
... INCOLOY ALLOY 802 is a high-carbon iron-base alloy recommended for high-temperature applications requiring excellent corrosion resistance and good mechanical properties. It is furnished in the annealed condition. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1993) 42 (12): SS-559.
Published: 01 December 1993
...: INCOLOY alloy 803 is the latest in the INCOLOY 800 series of alloy, all invented by lNC0 Alloys Intema- tional for service in the chemical, petrochemical, and thermal processing industries - 800,8GOH. 8OOH I@, 80 1, 802 and now 803. Alloy 803 has higher nickel and chro- mium contents than those of alloy...
Journal Articles
Alloy Digest (1984) 33 (9): Ni-302.
Published: 01 September 1984
... gas metal-arc (MIG) welding of INCONEL alloy 617. For extended service at temperatures above 1700 F(925 C). it is recommended for welding INCOLOY* alloy SOOH and 802. It also is recommended for welding a number of cast alloys. *lNCONEL and INCOLOY are registered trademarks for products of the INCO...
Journal Articles
Alloy Digest (1984) 33 (7): Ni-300.
Published: 01 July 1984
.... INCOLO\ alloy 800H and INCOLOY alloy 802. In addition. it is recommended for welding cast alloys IACI) such as HK-40. HP and HP-45 Modified. Manufacturer: Corrosion Resistance: INCONEL Welding Electrode I I7 provides excellent resistance IO cyclic oxidatton condittons at temperatures up IO 19tJV F (1040...