Alloy Digest (2010) 59 (3): SS-1056.
Published: 01 March 2010
... Incoloy alloy 25-6HN is a 6% Mo superaustenitic stainless steel. It offers an excellent combination of strength, ductility, and resistance to corrosion by a variety of media at an economical price. It is readily formed and welded. The properties of the alloy are enhanced by its content of nitrogen...