Alloy Digest (1996) 45 (10): Ni-517.
Published: 01 October 1996
... Inco-Weld Filler Metal 686CPT is a welding product with higher (Cr + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include welding many CRA materials for corrosive service...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... be by gas tungsten arc, gas metal arc, and shielded metal arc processes. Matched composition welding products, such as Inconel Welding Electrode 122 and Filler Metal 622, are available. Overmatching composition welds may be deposited with Inco-Weld Filler Metal 686CPT or Inco-Weld Welding Electrode 686CPT...
Journal Articles
Alloy Digest (1996) 45 (8): Ni-515.
Published: 01 August 1996
... Inco-Weld Welding Electrode 686CPT is an all-position shielded-metal-arc (SMAW) electrode with highter (CR + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1056.
Published: 01 March 2010
... of filler material. While alloy 25-6HN is normally joined with Inconel filler metal 625, a higher CPT results from the use of the more-resistant Inco-Weld 686CPT filler metal. Annealing after fabrication can also have a positive influence on the corrosion resistance of welded components. Table 3 Resistance...
Journal Articles
Alloy Digest (2003) 52 (1): SS-871.
Published: 01 January 2003
... of its corrosion resistance when autogenously welded or when welded with matching com- position filler metal. Overmatching composition welding products with higher molybdenum content are used such as Inconel Filler Metals 622, C-276, and 686CPT, Inconel Welding Electrodes 122 and C-276, and Inco-Weld...
Journal Articles
Alloy Digest (2021) 70 (3): Ni-768.
Published: 01 March 2021
.... Inco-Weld filler metal and welding electrode 686CPT can be used to overmatch 30 200 Inconel C-276 where enhanced corrosion resistance is Yield Strength required. 20 (0.2% Offset) 100 10 0 Comparable Grades 0 200 400 600 800 1000 1200 1400 1600 Temperature, ┬░F Special Metals Corporation ASTM Fig. 1...