Alloy Digest (1969) 18 (5): Zn-12.
Published: 01 May 1969
... ILZRO-12 is a zinc-base foundry alloy recommended for general purpose castings. It has economic advantages by virtue of lower material costs and a lower casting temperature than competitive copper-base alloys. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1972) 21 (5): Zn-14.
Published: 01 May 1972
... ILZRO 16 is a zinc-base die-casting alloy which was developed to have superior creep resistance at both ambient and elevated temperatures for processing in cold-chamber die-casting machines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1968) 17 (8): Zn-11.
Published: 01 August 1968
... ILZRO-14 is a zinc-base die casting alloy developed with superior creep resistance at both ambient and elevated temperatures. It is recommended for carburetors, fuel pumps, valve bodies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties...