1-20 of 120 Search Results for

ISO-CAST 8

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1968) 17 (10): SA-232.
Published: 01 October 1968
... ISO-CAST 8 is a cast chromium-molybdenum steel recommended as a general purpose structural alloy of wide application with wide range of mechanical properties. It is used for aircraft and railroad car parts, machine tool and hammermill equipment, gears and shafts. This datasheet provides...
Journal Articles
Alloy Digest (1967) 16 (5): SA-210.
Published: 01 May 1967
... ISO-CAST 9A is cast nickel-chromium-vanadium steel recommended as a structural alloy of high strength and impact resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating...
Journal Articles
Alloy Digest (2021) 70 (6): CI-82.
Published: 01 June 2021
... cast irons, which have inferior thermal properties Chemical Composition Casting Characteristics The chemical composition of ISO 185/JL/300 is left to the Property Unit Value discretion of the manufacturer, who shall adjust the compo- Minimum casting section thickness mm (in.) 10 (3/8) sition in order...
Journal Articles
Alloy Digest (2021) 70 (9): CI-85.
Published: 01 September 2021
... Supplier Annealing. Heat to 900 950 °C (1650 1740 °F) at 100 200 International Organization for Standardization (ISO) °C/h (180 360 °F/h). For thin section and fragile castings, ISO Central Secretariat reduce the heating rate to 50 100 °C/h (90 180 °F/h). Hold Chemin de Blandonnet 8 for 1 h plus 1 h per 25...
Journal Articles
Alloy Digest (2020) 69 (12): CI-76.
Published: 01 December 2020
... contraction Unit mm (in.) % mm/m (in./ft) Value 7 (9/32) 0.8 1.2 10 13 (1/10 1/8) (a) Depends upon design, size of casting and heat treatment. Source: Meehanite Specification Handbook, 2013 Heat Treatment ISO 185/JL/250 does not normally require heat treatment, except for remedial reasons. Table 3 Electrical...
Journal Articles
Alloy Digest (1972) 21 (8): SS-278.
Published: 01 August 1972
... Filing Code: ss-278 EMPIRE NO-40 Steinless Steel AUGUST 1972 - DATA ON WORLD WIDE METALS AND ALLOYS Pdlisbed by Engineering Alloys Digcn Inc. Upper Monakir, New Jew EMPIRE ISO-40* (High-Strength Cast Stainless Steel with Excellent Corrosion Resistance) EMPIRE IS040 is a precipitation-hardenable stainless...
Journal Articles
Alloy Digest (2020) 69 (9): CI-73.
Published: 01 September 2020
... ISO 185/JL/225 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 225–325 MPa (33-47 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray...
Journal Articles
Alloy Digest (2020) 69 (6): CI-70.
Published: 01 June 2020
... ISO 185/JL/200 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 200–300 MPa (29–44 ksi) when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray...
Journal Articles
Alloy Digest (2021) 70 (3): CI-79.
Published: 01 March 2021
... ISO 185/JL/275 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 275–375 MPa (40–54 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Journal Articles
Alloy Digest (1963) 12 (6): SA-147.
Published: 01 June 1963
... ISO-CAST 5 is a cast manganese-molybdenum steel of medium strength for general purposes. It is recommended for automobile and tractor parts, structural and machinery castings, gears, housings, etc. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2020) 69 (3): CI-67.
Published: 01 March 2020
... ISO 185/JL/150 is an unalloyed low-tensile-strength gray cast iron that has high carbon and silicon contents, and thus the highest thermal conductivity and damping capacity. It is, therefore, useful in situations where high thermal conductivity, damping capacity, and machinability are important...
Journal Articles
Alloy Digest (1972) 21 (5): SS-273.
Published: 01 May 1972
... EMPIRE ISO-450 is a cast stainless steel with excellent corrosion resistance. A simple, single-step aging treatment develops high strength with good ductility and toughness. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2023) 72 (5): CI-105.
Published: 01 May 2023
... Mechanical Properties See Tables 3 4. Design Stress See Table 5. Casting Characteristics Property Patternmaker s contraction(a) Solid contraction Unit % mm/m in/ft Value 0.2 to 0.8 8 1/32 to 3/32 Typical values. (a) Depends upon design, size of casting, and heat treatment applied, if any. Source: Meehanite...
Journal Articles
Alloy Digest (2020) 69 (5): Al-464.
Published: 01 May 2020
.... Quench in water at 50 80 °C (120 175 °F). Precipitation heat treatment Age at 160 175 °C (320 345 °F) for 6 7 h. Cool in still air. Age at 130 145 °C (265 295 °F) for 6 7 h. Cool in still air. Comparable Grades Ingots for Remelting Raffmetal S.p.A. EN 1676:2010 ISO 17615:2007 Castings Raffmetal S.p.A. EN...
Journal Articles
Alloy Digest (2022) 71 (9): CI-97.
Published: 01 September 2022
... mm (1.2 in.) diameter test bars. Source: ISO 185:2020, Grey cast irons Classification Table 3 Electrical and magnetic properties Property Unit At Value Electrical Resistivity m 20 °C circular-mil/ft) (68 °F) 0.70 (421) Coercivity A/m 20 °C 560 720 (Oe) (68 °F) (7.04 9.05) Maximum permeability...
Journal Articles
Alloy Digest (2020) 69 (3): Al-462.
Published: 01 March 2020
...-21000) ISO AB-Al Cu4MgTi AC1B.1 204.2 Castings Raffmetal S.p.A. EN 1706:2010 ISO 3522:2007 JIS H 5202:2010 ASTM B26/B26M:2018e1 ASTM B108/B108M:2019 EN AC-Al Cu4MgTi (EN AC-21000) EN AC-Al Cu4MgTi (EN AC-21000) ISO AC-Al Cu4MgTi AC1B 204.0 General Characteristics High strength and ductility, very high...
Journal Articles
Alloy Digest (2020) 69 (8): Al-467.
Published: 01 August 2020
... treatment: Age at 155 165 °C (310 330 °F) for 8 12 h. Cool in still air. Comparable Grades Ingots for Remelting Raffmetal S.p.A. EN 1676:2010 ISO 17615:2007 EN AB-Al Si2MgTi (EN AB-41000) EN AB-Al Si2MgTi (EN AB-41000) ISO AB-Al Si2MgTi Castings Raffmetal S.p.A. EN 1706:2010 ISO 3522:2007 EN AC-Al Si2MgTi...
Journal Articles
Alloy Digest (2021) 70 (9): Al-480.
Published: 01 September 2021
..., min Hardness, min % HBW Casting method Temper MPa ksi MPa ksi 2 75 Sand casting T6 4 60 T64 230 33 190 28 4 90 Shell mold T6 8 80 casting T64 200 29 120 17 290 42 210 30 250 36 180 26 T6 = solution heat treated and fully artificially aged; T64 = solution heat treated and artificially under aged...
Journal Articles
Alloy Digest (2022) 71 (2): CI-90.
Published: 01 February 2022
... circular-mil/ft) J/m3 At 20 °C (68 °F) 20 to 100 °C (68 to 392 °F) 200 °C (392 °F) 20 to 500 °C (68 to 932 °F) 20 °C (68 °F) 20 °C (68 °F) Value 7100 (0.256) 12.5 (6.90) 39 (23.8) 515 (0.123)(a) 0.50 (301)(a) 600(a) Typical values. (a) ISO 1083:2018, Spheroidal graphite cast irons Classification...
Journal Articles
Alloy Digest (2022) 71 (4): CI-92.
Published: 01 April 2022
... (25.2) 42.0 (24.3) 41.5 (24.0) 460 (0.110) 535 (0.128) Typical values. Measured on separately cast, 30 mm (1.2 in.) diameter test bars. Source: ISO 185:2020, Grey cast irons Classification Table 3 Electrical and magnetic properties Property Electrical resistivity Coercivity Maximum permeability...