1-18 of 18

Search Results for ISO 185/JL/300

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2021) 70 (6): CI-82.
Published: 01 June 2021
... ISO 185/JL/300 is a higher-tensile-strength gray cast iron that has a pearlitic matrix; it has a tensile strength of 300–400 MPa (44–58 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. It provides high strength while still maintaining good...
Journal Articles
Alloy Digest (2020) 69 (6): CI-70.
Published: 01 June 2020
... ISO 185/JL/200 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 200–300 MPa (29–44 ksi) when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray...
Journal Articles
Alloy Digest (2021) 70 (9): CI-85.
Published: 01 September 2021
... the use of one of the other higher-strength materials such as spheroidal graphite cast irons, which have inferior thermal properties. Chemical Composition Table 2 Density and thermal properties The chemical composition of ISO 185/JL/300 is left to the Property Unit At Value discretion of the manufacturer...
Journal Articles
Alloy Digest (2022) 71 (9): CI-97.
Published: 01 September 2022
... treatment sourced from ISO/TR 108091:2009, Cast irons Part 1: Materials and properties for design. Comparable Grades JIS G 5501:1995 ASTM A48/A48M:2003(2021) EN 1561:2011 ISO 185:2020 SAE J431:2018 FC300 Class 300B EN-GJL-300 (5.1302) ISO 185/JL/300 G13H22 General Characteristics Good thermal conductivity...
Journal Articles
Alloy Digest (2020) 69 (11): CI-75.
Published: 01 November 2020
...) Comparable Grades Meehanite Metal Corporation ASTM A48/A48M:2003(2016) EN 1561:2011 ISO 185:2020 JIS G 5501:1995 Meehanite GB300 Class 300B EN-GJL-300 (5.1302) ISO 185/JL/300 FC300 General Characteristics Meehanite GB300 is a heat-treatable gray cast iron that is characterized by excellent hardenability...
Journal Articles
Alloy Digest (2020) 69 (12): CI-76.
Published: 01 December 2020
... ISO 185/JL/250 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 250–350 MPa (36–51 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Journal Articles
Alloy Digest (2020) 69 (9): CI-73.
Published: 01 September 2020
... ISO 185/JL/225 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 225–325 MPa (33-47 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray...
Journal Articles
Alloy Digest (2020) 69 (3): CI-67.
Published: 01 March 2020
... ISO 185/JL/150 is an unalloyed low-tensile-strength gray cast iron that has high carbon and silicon contents, and thus the highest thermal conductivity and damping capacity. It is, therefore, useful in situations where high thermal conductivity, damping capacity, and machinability are important...
Journal Articles
Alloy Digest (2021) 70 (3): CI-79.
Published: 01 March 2021
... ISO 185/JL/275 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 275–375 MPa (40–54 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Journal Articles
Alloy Digest (2022) 71 (4): CI-92.
Published: 01 April 2022
... 185:2020 FC350 Class 350B EN-GJL-350 (5.1303) ISO 185/JL/350 Table 6 Maximum allowable design stress at room temperature Stress condition Direct tension Direct compression Fatigue, rotating bending Fatigue, push-pull Maximum allowable design stress MPa ksi 88(a) 13(a) 182(b) 26(b) 53(c) 8(c) 40(c) 6(c...
Journal Articles
Alloy Digest (2021) 70 (5): CI-81.
Published: 01 May 2021
... the quenching bath while above 150 °C (300 °F) and tem- Class 250B per immediately. Meehanite Metal Corporation ASTM A48/A48M:2003(2016) EN-GJL-250 (5.1301) Surface Hardening. Surface hardness values in excess of 500 EN 1561:2011 ISO 185/JL/250 HBW can be obtained by flame, induction, or laser harden- ISO 185...
Journal Articles
Alloy Digest (2022) 71 (8): CI-96.
Published: 01 August 2022
.../h (90 °F/h). Continue cooling in still air. I n formation on heat treatment sourced from ISO/TR 10809-1:2009. Comparable Grades EN 1561:2011 ASTM A48/A48M:2003(2021) ISO 185:2020 JIS G 5501:1995 SAE J431:2018 EN-GJL-200 (5.1300) Class 200B ISO 185/JL/200 FC200 G10H18 CI-96 / 2 Table 6 Maximum...
Journal Articles
Alloy Digest (2021) 70 (11): CI-87.
Published: 01 November 2021
... Other mechanical properties ASTM A48/A48M:2003(2016) Meehanite GE200 EN 1561:2011 Class 200B Property Unit Value ISO 185:2020 0.1% proof strength(a) MPa (ksi) 130 195 (18.86 28.28) JIS G 5501:1995 EN-GJL-200 (5.1300) 0.1% proof strength in MPa (ksi) SAE J431:2018 ISO 185/JL/200 compression 260 (37.70...
Journal Articles
Alloy Digest (2020) 69 (8): CI-72.
Published: 01 August 2020
.... Comparable Grades Meehanite Metal Corporation ASTM A48/A48M:2003(2016) EN 1561:2011 ISO 185:2020 JIS G 5501:1995 Meehanite GA350 Class 350B EN-GJL-350 (5.1303) ISO 185/JL/350 FC350 General Characteristics High strength, toughness, wear resistance, and damping capacity; good thermal conductivity...
Journal Articles
Alloy Digest (2021) 70 (2): CI-78.
Published: 01 February 2021
... by flame, induction, or laser harden- ISO 185:2020 ing. While there is no practical limit to the depth of hardness SAE J431:2018 ISO 185/JL/275 that can be achieved, it is generally accepted that depths of G12H21, G13H19 hardness of up to 6 mm (0.25 in.) can be obtained. Beyond this depth, the dangers...
Journal Articles
Alloy Digest (2021) 70 (8): CI-84.
Published: 01 August 2021
... Hardening. Preheat slowly to 590 °C (1100 °F). Raise ASTM A48/A48M:2003(2016) ISO 185/JL/225 the temperature to 850 900 °C (1560 1650 °F) as quickly as ISO 185:2020 G10H21, G11H18 possible. Wait for equalization of the temperature. Soak for 1 SAE J431:2018 h per 25 mm (1 in.) of maximum section thickness...
Journal Articles
Alloy Digest (2022) 71 (3): CI-91.
Published: 01 March 2022
...:1995 SAE J431:2018 EN-GJL-150 (5.1200) Class 150B ISO 185/JL/150 FC150 G9H12 General Characteristics Very high thermal conductivity; very high damping capacity; low tensile strength; very high machinability. Product Forms Castings manufactured in sand molds or in molds with comparable thermal behavior...
Journal Articles
Alloy Digest (2022) 71 (2): CI-90.
Published: 01 February 2022
... is much greater than that of Meehanite GA350 gray cast iron ( ISO 185/JL/350); good impact properties at low temperature; machinability is inferior to that of gray cast iron; weldability is superior to that of gray cast iron. Applications Parts for compressors, pumps, refrigerators, valves etc., which...