Alloy Digest (2021) 70 (3): CI-79.
Published: 01 March 2021
... ISO 185/JL/275 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 275–375 MPa (40–54 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Journal Articles
Alloy Digest (2021) 70 (2): CI-78.
Published: 01 February 2021
... flame, induction, or laser harden- ISO 185:2020 ing. While there is no practical limit to the depth of hardness SAE J431:2018 ISO 185/JL/275 that can be achieved, it is generally accepted that depths of G12H21, G13H19 hardness of up to 6 mm (0.25 in.) can be obtained. Beyond this depth, the dangers of...
Journal Articles
Alloy Digest (2020) 69 (8): CI-72.
Published: 01 August 2020
... rods. Comparable Grades Meehanite Metal Corporation Meehanite GA350 ASTM A48/A48M:2003(2016) Class 350B EN 1561:2011 EN-GJL-350 (5.1303) ISO 185:2020 ISO 185/JL/350 JIS G 5501:1995 FC350 General Characteristics High strength, toughness, wear resistance, and damping capacity; good thermal conductivity...
Journal Articles
Alloy Digest (2021) 70 (5): CI-81.
Published: 01 May 2021
...×lbf) 4.9 (3.7) 10 20 0.375 0.750 MPa ksi MPa ksi HBW 20 40 0.750 1.625 40 80 1.625 3.250 275 39.9 270 240 34.8 250 (a) Determined on 30 mm (1.2 in.) separately cast test bars at 20 °C (68 °F). (b) Source: ISO 185:2020. (c) Unnotched test piece. (d) Unnotched Charpy test piece (10 mm, or 230 33.4...