Alloy Digest (2020) 69 (9): CI-73.
Published: 01 September 2020
... ISO 185/JL/225 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 225–325 MPa (33-47 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray...
Journal Articles
Alloy Digest (2021) 70 (8): CI-84.
Published: 01 August 2021
... Hardening. Preheat slowly to 590 °C (1100 °F). Raise ASTM A48/A48M:2003(2016) ISO 185/JL/225 the temperature to 850 900 °C (1560 1650 °F) as quickly as ISO 185:2020 G10H21, G11H18 possible. Wait for equalization of the temperature. Soak for 1 SAE J431:2018 h per 25 mm (1 in.) of maximum section thickness...
Journal Articles
Alloy Digest (2020) 69 (12): CI-76.
Published: 01 December 2020
... ISO 185/JL/250 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 250–350 MPa (36–51 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Journal Articles
Alloy Digest (2021) 70 (6): CI-82.
Published: 01 June 2021
... 3.15 225 33 210 30 80 150 3.15 5.91 210 30 195 28 150 300 5.91 11.8 190 28 185 27 Table 5 Other mechanical properties at room Information on heat treatment sourced from ISO/TR 10809- temperature 1:2009, Table 7. Property Unit Value Comparable Grades ISO 185/JL/300 MPa (ksi) 300 400 (44 58) Class 300B...
Journal Articles
Alloy Digest (2022) 71 (4): CI-92.
Published: 01 April 2022
... 185:2020 FC350 Class 350B EN-GJL-350 (5.1303) ISO 185/JL/350 Table 6 Maximum allowable design stress at room temperature Stress condition Direct tension Direct compression Fatigue, rotating bending Fatigue, push-pull Maximum allowable design stress MPa ksi 88(a) 13(a) 182(b) 26(b) 53(c) 8(c) 40(c) 6(c...
Journal Articles
Alloy Digest (2020) 69 (8): CI-72.
Published: 01 August 2020
.... Comparable Grades Meehanite Metal Corporation ASTM A48/A48M:2003(2016) EN 1561:2011 ISO 185:2020 JIS G 5501:1995 Meehanite GA350 Class 350B EN-GJL-350 (5.1303) ISO 185/JL/350 FC350 General Characteristics High strength, toughness, wear resistance, and damping capacity; good thermal conductivity...
Journal Articles
Alloy Digest (2022) 71 (2): CI-90.
Published: 01 February 2022
... is much greater than that of Meehanite GA350 gray cast iron ( ISO 185/JL/350); good impact properties at low temperature; machinability is inferior to that of gray cast iron; weldability is superior to that of gray cast iron. Applications Parts for compressors, pumps, refrigerators, valves etc., which...
Journal Articles
Alloy Digest (2021) 70 (2): CI-78.
Published: 01 February 2021
... by flame, induction, or laser harden- ISO 185:2020 ing. While there is no practical limit to the depth of hardness SAE J431:2018 ISO 185/JL/275 that can be achieved, it is generally accepted that depths of G12H21, G13H19 hardness of up to 6 mm (0.25 in.) can be obtained. Beyond this depth, the dangers...