Alloy Digest (1981) 30 (9): Bi-26.
Published: 01 September 1981
... INDALLOY 117 is a bismuth-base, eutectic alloy that has a melting point of 117 F (47 C). Because of its low melting temperature and controlled-shrinkage characteristics, it is used widely in industry. The alloy can be recovered easily and recycled into new uses any number of times. Its many uses...