Alloy Digest (2014) 63 (8): Ni-716.
Published: 01 August 2014
...-temperature alloys INCONEL alloy 740H joinability machinability physical properties steam boilers tensile properties workability DATA ON WORLDWIDE METALS AND ALLOYS Published by: ASM International Data shown are typical, not to be used for specification or final design. Materials Park, OH 44073-0002...
Journal Articles
Alloy Digest (2020) 69 (9): Ni-762.
Published: 01 September 2020
... Special Metals Inconel 740H (UNS N07740) is a precipitation hardenable, nickel-base superalloy that offers a unique combination of high strength and creep resistance at elevated temperatures along with resistance to coal ash corrosion. This alloy was originally targeted for use in advanced ultra...