Alloy Digest (1972) 21 (7): Ni-176.
Published: 01 July 1972
... INCONEL alloy 600 (formerly INCONEL, Alloy Digest Ni-9, March 1954) is a nickel-chromium-iron alloy with good resistance to corrosion and heat. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with a desirable combination of high...
Journal Articles
Alloy Digest (2020) 69 (4): Ni-758.
Published: 01 April 2020
... Special Metals Inconel Alloy 600 (UNS N06600 / Werkstoff Number 2.4816) is a nickel-chromium-iron alloy that is intended for corrosion-resistant and heat-resistant applications. Its versatility has led to its use in a variety of applications involving temperatures from cryogenic to above 1095 °C...
Journal Articles
Alloy Digest (1960) 9 (3): Ni-56.
Published: 01 March 1960
... INCONEL 600 nickel-base alloy has better high temperature properties than Inconel alloy, particularly where rupture strength, creep and short-time tensile are necessary. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1986) 35 (11): Ni-342.
Published: 01 November 1986
... INCONEL Filler Metal 82 is used for gas-tungsten-arc, gas-metal-arc, and submerged-arc welding of INCONEL alloys 600, 601 and 690, INCOLOY alloys 800 and 800H, and INCO alloy 330. It also is used for surfacing of steel. Dissimilar-welding applications for which the filler metal is used include...
Journal Articles
Alloy Digest (1985) 34 (11): Ni-325.
Published: 01 November 1985
... INCONEL Welding Electrode 182 is used for shielded-metal-arc welding of INCONEL alloys 600, 601 and 690. Dissimilar welds for which the electrode is used include INCONEL and INCOLOY alloys joined to carbon steels, stainless steels, nickel and MONEL alloys; MONEL alloys joined to carbon steels...
Journal Articles
Alloy Digest (1986) 35 (4): Ni-331.
Published: 01 April 1986
... INCONEL Filler Metal 62 is used for gas-tungsten-arc, gas-metal-arc and oxyacetylene welding of INCONEL alloy 600 in thicknesses up to 2 inch (50 mm). The weld metal is comparable to the base metal in high-temperature strength and oxidation resistance. For material over 2-inch (50-mm) thick...
Journal Articles
Alloy Digest (1985) 34 (10): Ni-323.
Published: 01 October 1985
... IONCONEL Welding Electrode 132 is used for shielded-metal-arc welding of INCONEL alloys 600 and 601 and INCO alloy 330. Electrode 132 has good dissimilar-welding capability. Examples are joining INCONEL and INCOLOY alloys to carbon steels, stainless steels, nickel and MONEL alloys. It also is used...
Journal Articles
Alloy Digest (1984) 33 (11): Ni-305.
Published: 01 November 1984
... INCO-WELD A Electrode is a nickel-base alloy developed for shielded metal-arc welding of INCONEL alloys 600 and 601 and INCOLOY alloy 800H to be exposed to elevated temperatures (up to about 1600 F). This electrode also is used widely for various dissimilar combinations of austenitic and ferritic...
Journal Articles
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
... cold forming is similar to that of INCONEL alloy 600. Somewhat higher forces, however, are required for alloy 690. The work-hardening rate of alloy 690 is similar to those of AISI Type 304 stainless steel and INCONEL alloy 600. INCONEL alloy 690 is readily fabricated by conven- tional techniques...
Journal Articles
Alloy Digest (2002) 51 (6): Ni-584.
Published: 01 June 2002
...: 10.31399/asm.ad.ni0584 General Characteristics: Rima 82 filler metal is used for gas tungsten arc, gas metal arc, and submerged arc welding of Inconel alloys 600, 601, and 690, alloys 800 and 800H, and alloy 330. It also is used for surfacing of steel. Dissimilar welding applications for which the filler...
Journal Articles
Alloy Digest (1967) 16 (2): Ni-121.
Published: 01 February 1967
...-ion stress-corrosion cracking and resists oxidation and a broad spectrum of corrosive environments. Results of cyclic oxidation tests performed on this alloy are compared below with rhose of INCONEL alloy 600. CYCLIC OXIDATION Hours of Change in Weight, % 18OOOF 2000OF INCONEL alloy 625 is a nickel...
Journal Articles
Alloy Digest (1974) 23 (10): Ni-210.
Published: 01 October 1974
... and elevated temperature. Its general corrosion resistance is equivalent to that of INCONEL* alloy 600. Colmonoy No. 72 has good resistance to chemical corrosion, scaling at high temperatures and fretting corrosion at high temperatures. Likewise, its general corrosion resistance is equivalent to INCONEL alloy...
Journal Articles
Alloy Digest (1994) 43 (5): Ni-453.
Published: 01 May 1994
... and vacuum atmospheres. NICROBELL C. with its higher chromium content is used in carburizing environments. It is more resistant to carburizing and sulfidizing atmospheres than INCONEL@ alloys 600 and 601. @INCONEL is a trademark of the Into family of companies. Available Product Forms: Sheathing on mineral...
Journal Articles
Alloy Digest (1986) 35 (3): Ni-329.
Published: 01 March 1986
...® 1996 hardenable alloys and is recommended for INCONEL alloy 600 and Nickel 200 to impart maximum corrosion resistance in caustic soda. Except for age-hardenabie alloys, cooling rate after welding is not important for nickel alloys. Extremes of slow cooling and water quenching can be used without...
Journal Articles
Alloy Digest (2003) 52 (11): Ni-617.
Published: 01 November 2003
... quenching. Consult the manufacturer for the recommended quenching method that is dependent on section thickness. Fabricability: This alloy is readily fabricated by conventional techniques. Its forming and machining characteristics are similar to those of INCONEL alloy 600 or 690. Alloy 693 is joined...
Journal Articles
Alloy Digest (1986) 35 (6): Ni-333.
Published: 01 June 1986
.... Postweld stress relief, which is usually required for low-alloy and carbon steels, is generally not required for nickel alloys. Stress relief may be necessary forage- hardenable alloys and is recommended for INCONEL alloy 600 to impart maximum corrosion resistance in caustic soda. Except for age-hardenable...
Journal Articles
Alloy Digest (1976) 25 (5): Ni-227.
Published: 01 May 1976
... not be used in sodium sulfite liquor and lactic acid (miIk products). It has corrosion resistance, in general, slmiIar to that of INCONEL alloy 600. (INCONEL is a registered trademark of The International Nickel co., Inc.) Specification Equivalents: Colmonoy No. 42SA meets the requirements of AWS-A5.13-70...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-313.
Published: 01 April 1985
... not required for nickel alloys. Stress relief may be necessary forage- hardenable alloys and is recommended for INCONEL alloy 600 and Nickel 200 to impart maximum corrosion resistance in caustic soda. Except for age-hardenable alloys, cooling rate after welding is not important for nickel alloys. Extremes...
Journal Articles
Alloy Digest (1984) 33 (7): Ni-300.
Published: 01 July 1984
... diameter (See Table I ). Applications: INCONEL Welding Electrode I I7 is used for all-positton shielded metal-arc welding of INCONEL alloy 617. II is also recommended for the welding of dissimilar wrought materials such as INCONEL alloy 600. INCONEL alloy 601. INCOLO\ alloy 800H and INCOLOY alloy 802...
Journal Articles
Alloy Digest (1975) 24 (12): Ni-222.
Published: 01 December 1975
... corrosion alone. It is not resistant to ferric chloride and hot or concentrated hydrochloric acid. Also, it should not be used in sodium sulfite liquor and lactic acid (milk products). It has corrosion resistance, in general, similar to that of INCONEL alloy 600. (INCONEL is a reeistered trademark...