Alloy Digest (1986) 35 (4): Ni-331.
Published: 01 April 1986
... INCONEL Filler Metal 62 is used for gas-tungsten-arc, gas-metal-arc and oxyacetylene welding of INCONEL alloy 600 in thicknesses up to 2 inch (50 mm). The weld metal is comparable to the base metal in high-temperature strength and oxidation resistance. For material over 2-inch (50-mm) thick...
Journal Articles
Alloy Digest (1992) 41 (5): Ni-403.
Published: 01 May 1992
...- loys. Hot forming should be done in the range 1750- 2100°F (955-1150°C). Weldability: Into alloy 330 is weldable by conventional processes. When shielded-metal-arc welding, use INCO-WELD* A Electrode or INCONEL* Welding Electrode 132. Gas- shielded-arc welding is done with INCONEL Filler Metal 62 or 82...
Journal Articles
Alloy Digest (1991) 40 (1): Ni-391.
Published: 01 January 1991
..., and soldering processes. Welding materials for joining are INCONEL Welding Elec- trodes 132 and 182 for shielded metal-arc welding; INCONEL Filler Metals 62 and 82 for gas tungsten-arc, gas metal-arc, and submerged-arc welding; and INCONEL Fiier Metal 62 for oxyacetylene welding. INCOFLUX 4 Submerged Arc Flux...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
...: The deposited weld metal from 62-50 can be machined success- fully by following the normal procedures used for nickel alloys. The machinability of weldments will vary with the base metal and the amount of dilution. Consult the filler metal manufacturer for more details. Corrosion Resistance: The weld metal...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... be by gas tungsten arc, gas metal arc, and shielded metal arc processes. Matched composition welding products, such as Inconel Welding Electrode 122 and Filler Metal 622, are available. Overmatching composition welds may be deposited with Inco-Weld Filler Metal 686CPT or Inco-Weld Welding Electrode 686CPT...
Journal Articles
Alloy Digest (2009) 58 (3): Ni-667.
Published: 01 March 2009
... exhibits good weldability. Inconel Filler Metals 617 and 230 are used for gas tungsten arc (GTA) and gas metal arc (GMA) welding. Inconel Welding Electrode 117 is used for shielded metal arc (SMA) welding. Dissimilar welding applications are best accomplished with Inconel filler metal 617 and Inconel...
Journal Articles
Alloy Digest (2003) 52 (8): Ni-611.
Published: 01 August 2003
...), and submerged metal arc (SMAW). For applications requiring high strength and resistance to creep and stress rupture, Inconel Filler Metal 617 and Inconel Welding Electrode 117 should be used. When resistance to high-tempera- ture corrosion is critical, Inconel Filler Metal 52 and Inconel Welding Electrode 152...
Journal Articles
Alloy Digest (2010) 59 (1): Ni-639.
Published: 01 January 2010
.... Inconel Welding Electrode 117 is used for shielded metal arc (SMA) welding. Dissimilar welding applications are best accomplished with Inconel Filler Metal 617 and Inconel Welding Electrode 117. Corrosion Resistance: This alloy is designed to o er resistance to a variety of corrosion mechanisms at high...
Journal Articles
Alloy Digest (1958) 7 (3): Ni-40.
Published: 01 March 1958
... is about 65%. Weldability: Can be metal arc welded using 132 Inconel or 139 Inconcl X electrodes. Care must be exercised to re- move all welding slag. The inert gas tungsten arc pro- cess is preferred using filler metal of matching composi- tion or as alternates, 62 Inconel or 69 Inconel X...
Journal Articles
Alloy Digest (1957) 6 (11): SS-64.
Published: 01 November 1957
...: Cannot be hardened by any thermal treatment. Can be hardened by cold working only. Weldability: Incoloy-T can be welded by standard metal arc and inert gas merhods. Use 132 Inconel electrode for metal arc welding this alloy. If desirable to use inert gas metal arc welding, 62 Inconel filler wire...
Journal Articles
Alloy Digest (2021) 70 (3): Ni-768.
Published: 01 March 2021
.... Inco-Weld filler metal and welding electrode 686CPT can be used to overmatch 30 200 Inconel C-276 where enhanced corrosion resistance is Yield Strength required. 20 (0.2% Offset) 100 10 0 Comparable Grades 0 200 400 600 800 1000 1200 1400 1600 Temperature, °F Special Metals Corporation ASTM Fig. 1...
Journal Articles
Alloy Digest (1960) 9 (9): Ni-60.
Published: 01 September 1960
... Inconel electrode is recommended for metal-arc welding while 62 Inconel filler wire is recom- mended for inert gas process. For oxyacetylene welding used 42 Inconel filler wire with Into 2 gas welding flux. Neither preweld nor post- weld heat treating: is required. Corrosion Resistance: It has...
Journal Articles
Alloy Digest (1967) 16 (1): Ni-120.
Published: 01 January 1967
... and under using Inconel 62 filler metal and short arc. Oxyacetylene gas welding is applicable to material thickness of 0.125 and under, using Inconel 42 filler metal wire, No. 2 flux, and slightly reducing flame. Most coared electrodes for metal arc welding contain fluorides in the flux coating...
Journal Articles
Alloy Digest (1967) 16 (10): SS-201.
Published: 01 October 1967
... Welding Electrode 182 for metal arc welding this alloy. If desirable to use inert gas metal arc welding. INCONEL Filler Metal 82 is recommended. At the present time the inert gas metal arc welding process is recommended for sheet and strip up to / inch thick only. After welding, no thermal or chemical...
Journal Articles
Alloy Digest (1999) 48 (8): SS-758.
Published: 01 August 1999
... austenitic/ferritic stainless steel with a designed pitting resistance equivalent number (PREN) of 34. URANUS is a registered trademark of Creusot-Loire Industrie. INCONEL is a registered trademark of Special Metal Corp. Chemical Composition, wt (Typical) Carbon 0.020 Chromium 22.5 Nickel 5.8 Molybdenum 3.1...
Journal Articles
Alloy Digest (1954) 3 (5): Ni-10.
Published: 01 May 1954
... a temperature of about 2000 deg. F. Weldability: FUSION WELDING: Can be welded by argon arc anJ oxy- accrylenc merhods using N.C. 82 as filler wire. A boron-free flux is required wirh rhe larrer process. hletallic arc welding can be used on thicker section using Inconel X electrodes. The High temperature...