1-2 of 2 Search Results for

INCONEL ALLOY MA 754

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1990) 39 (3): Ni-244.
Published: 01 March 1990
... Inconel alloy MA 754 is an oxide-dispersion-strengthened nickel-chromium alloy produced by mechanical alloying. It offers the advantages of a wrought high-temperature material in service environments where only cast alloys could be used in the past. Its strength in conjunction with its high...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-511.
Published: 01 May 1996
... Inconel alloy MA 758 is a further development of the well-established aerospace superalloy Inconel alloy MA 754 (Alloy Digest Ni-244, March 1990) with an increased chromium content for better resistance to high-temperature corrosives. This datasheet provides information on composition, physical...