Journal Articles
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
... INCONEL Alloy 690 is a wrought nickel-base alloy with excellent resistance to many corrosive aqueous media and high-temperature atmospheres. It also has high strength, good metallurgical stability, and favorable fabrication characteristics. It has excellent resistance to stress-corrosion cracking...
Journal Articles
Alloy Digest (2003) 52 (11): Ni-617.
Published: 01 November 2003
... This alloy improves upon the excellent high-temperature corrosion resistance of INCONEL alloy 690 (see Alloy Digest Ni-266, March 1981) through an addition of aluminum. Inconel Alloy 693 is typically 61% Ni, 29% Cr, 3.3% Al, and 0.7% Nb, with the balance being principally iron. By virtue of its...
Journal Articles
Alloy Digest (1992) 41 (7): Ni-406.
Published: 01 July 1992
... INCONEL WELDING ELECTRODE 152 is a high chromium rod for shielded-metal-arc welding of Inconel Alloy 690 (Alloy Digest Ni-266, March 1981). Higher chromium is beneficial in resisting stress-corrosion cracking in high purity water for pressurized water reactors and for resistance to oxidizing acids...
Journal Articles
Alloy Digest (1992) 41 (9): Ni-412.
Published: 01 September 1992
... INCONEL FILLER METAL 52 is a high chromium filler metal for gas-metal-arc and gas-tungsten-arc welding of Inconel Alloy 690 (See Alloy Digest Ni-266, March 1981). Higher chromium is beneficial in resisting stress-corrosion cracking in high purity water for pressurized water reactors...
Journal Articles
Alloy Digest (2003) 52 (7): Ni-610.
Published: 01 July 2003
... INCONEL Filler Metal 52M is a second-generation filler metal developed to weld Inconel alloy 690. Filler Metal 52M is used for repair in nuclear reactor systems in both similar and dissimilar welding. This datasheet provides information on composition, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (2021) 70 (6): Ni-771.
Published: 01 June 2021
... = room temperature. (a) At 15.9 kA/m (200 Oe). Source: Inconel Alloy 690, Special Source: Inconel Alloy 690, Special Metals Corporation, 2009 Metals Corporation, 2009 httpsdoi.org/10.31399/asm.ad.ni0771 Copyright © 2021, ASM International®. All rights reserved. chloride containing solutions, high...
Journal Articles
Alloy Digest (1986) 35 (11): Ni-342.
Published: 01 November 1986
... INCONEL Filler Metal 82 is used for gas-tungsten-arc, gas-metal-arc, and submerged-arc welding of INCONEL alloys 600, 601 and 690, INCOLOY alloys 800 and 800H, and INCO alloy 330. It also is used for surfacing of steel. Dissimilar-welding applications for which the filler metal is used include...
Journal Articles
Alloy Digest (1985) 34 (11): Ni-325.
Published: 01 November 1985
... INCONEL Welding Electrode 182 is used for shielded-metal-arc welding of INCONEL alloys 600, 601 and 690. Dissimilar welds for which the electrode is used include INCONEL and INCOLOY alloys joined to carbon steels, stainless steels, nickel and MONEL alloys; MONEL alloys joined to carbon steels...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-410.
Published: 01 August 1992
... INCONEL ALLOY 601GC is a nickel-chromium-iron alloy with additions of aluminum, zirconium, and nitrogen to resist oxidation and micro-alloy, the last to pin the grain boundaries and prevent grain growth at high temperatures. Maintaining finer grain sizes especially helps low cycle fatigue life...
Journal Articles
Alloy Digest (2013) 62 (1): Ni-706.
Published: 01 January 2013
... Products Corporation Copyright © ASM International® 2013 2013 ASM International chemical composition ductility heat treatability Inconel Filler Metal 52MSS joinability tensile properties workability UNS N06055 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®...
Journal Articles
Alloy Digest (1987) 36 (4): Ni-347.
Published: 01 April 1987
... INCONEL Welding Electrode 113 is used for shielded-metal-arc welding of alloy steels such as 5% nickel steel and 9% nickel steel for cryogenic applications. The weld metal has high mechanical properties, including impact values, at temperatures as low as -320 F (-196 C). Electrode 113 can...
Journal Articles
Alloy Digest (1992) 41 (11): Ni-416.
Published: 01 November 1992
...°F (595 C)/300 h - - 120 827 600 - 110 758 7ooo 10 loo 100 690 14 500 69 928 90 621 300 ooo >lO ooo ooo 80 552 1900000 >lO ocxl ooo 70 483 >lO ooo ooo - * Fbll/pull tests with 5OtXJ psi (34MPa) base stress. Mechanical Properties: INCONEL alloy 625LCF is produced in the annealed temper...
Journal Articles
Alloy Digest (2020) 69 (4): Ni-758.
Published: 01 April 2020
... Special Metals Inconel Alloy 600 (UNS N06600 / Werkstoff Number 2.4816) is a nickel-chromium-iron alloy that is intended for corrosion-resistant and heat-resistant applications. Its versatility has led to its use in a variety of applications involving temperatures from cryogenic to above 1095 °C...
Journal Articles
Alloy Digest (2002) 51 (6): Ni-584.
Published: 01 June 2002
...: 10.31399/asm.ad.ni0584 General Characteristics: Rima 82 filler metal is used for gas tungsten arc, gas metal arc, and submerged arc welding of Inconel alloys 600, 601, and 690, alloys 800 and 800H, and alloy 330. It also is used for surfacing of steel. Dissimilar welding applications for which the filler...
Journal Articles
Alloy Digest (1994) 43 (11): Ni-471.
Published: 01 November 1994
... INCONEL alloy 718SPF is an age-hardenable austenitic material whose strength is largely dependent on the precipitation of a gamma prime phase following heat treatment. The base alloy, however, possesses two-essential characteristics for super-plastic forming; grain size stability over time...
Journal Articles
Alloy Digest (2008) 57 (1): Ni-657.
Published: 01 January 2008
... Werkstoff Nr. 2.4886 BS 2901 NA48 DIN 1736 SG-NiMo16Cr16W EN ISO 18274 SNi6276 (NiCr15Mo16Fe6W4) For manufacture to ASME III (NCA3800, NB2400) and other specification, contact the producer. General Characteristics: This alloy is used for the gas tungsten arc and gas metal arc welding of Inconel alloy C-276...
Journal Articles
Alloy Digest (2019) 68 (8): Ni-754.
Published: 01 August 2019
... or final design. General Characteristics Inco-Weld C-276 Welding Electrode is used for shielded- metal-arc welding of Inconel alloy C-276 and other nickel-chromium-molybdenum alloys. It is also used for surfacing of steel. The weld metal has excellent corrosion resistance in many media and is especially...
Journal Articles
Alloy Digest (1998) 47 (6): Ni-543.
Published: 01 June 1998
... Sizes: INCO-CORED 82 flux cored wires are available at 1.1 mm (0.045 in.) diameter on 13.6 kg (30 lb) spools. Applications: lNCO-CORED 82DH and 82AP flux cored wires are recom- mended for a variety of welding applications, includiig: Joining INCONEL alloys 600.601, and 690; INCOLOY al- loys 800, 8OOH...
Journal Articles
Alloy Digest (1992) 41 (4): Ni-401.
Published: 01 April 1992
.... Welding: Using controlled welding procedures, weldments can be produced in lNC0 alloy 25-6M0 which exhibit excellent corrosion resistance. Use INCONEL alloy 625 filler metal withoveimatchingmolybdenumcontent(about9Lower welding speeds and greater puddling will create better mixing of elements...
Journal Articles
Alloy Digest (2007) 56 (1): Ni-646.
Published: 01 January 2007
... ranging from seawater to phosphoric acid. Inconel is a registered trademark of the Special Metals Group of Companies. Mechanical Properties: Hardness, HV 117 198 Yield strength, 0.2%, MPa (ksi) 280 ( 41) Tensile strength, MPa (ksi) 690 ( 100) Elongation, on 50 mm, % 40 Young s modulus, GPa (106 psi...