Journal Articles
Alloy Digest (1993) 42 (1): Ni-421.
Published: 01 January 1993
... INCONEL ALLOY 686 has a higher Cr + Mo + W content than the current generation of corrosion-resistant nickel-base alloys and exhibits improved corrosion resistance over them. The alloy could be used in reducing mineral acids and FGD equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1996) 45 (10): Ni-517.
Published: 01 October 1996
.... They are useful forjoining duplex. superduplex. and superaustenitic stain- less steels. for example. Into alloy 25-6MO and UNS N08367. NG6920, lnco alloy C-276. and Inconel alloys 622.625. and 686. 0 INCNEID INCONEl NW22 MC0 LwFe INmEt WkMetal Fww W!uMal INmEL RlerMenl 666cPT 622 G276 FiwNe!A 625 625 F% 1...
Journal Articles
Alloy Digest (2003) 52 (2): Ni-602.
Published: 01 February 2003
... N06059 DIN 2.4605 (NiCr23Mo16Al) Proprietary Nicrofer 5923hMo (Krupp VDM) Proprietary Inconel alloy 686 (Special Metals) + W Proprietary Hastelloy alloy C2000 (Haynes) + Cu Alloy C22 and similar ASTM/UNS N06022 ASTM/UNS A494 Grade CX2MW (cast) DIN 2.4602 (NiCr21Mo14W) DIN 2.4811, 2.4836 (NiCr20Mo15) DIN...
Journal Articles
Alloy Digest (1996) 45 (8): Ni-515.
Published: 01 August 1996
... combina- tion. in the test media was Inconel alloy 686 welded with the 686CPT consumables. The new 686CPT consumables are also capable of being used to deposit overlays of outstanding corrosion resistance onto a range of steels, using standard welding techniques. Tensile properties are: Tensile strength...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-596.
Published: 01 December 2002
..., typical, wt % Fe Mn Ni Cr Mo Cu F OES (mg/m3) 1 4 10 5 6 0.2 16 1 OES, occupational exposure standard limit Table 3 Materials to be Welded ASTM/UNS DIN Proprietary Alloy 59 and similar N06059 2.4605 (NiCr23Mo16Al) Nicrofer 5923hMo (Krupp VDM), Inconel Alloy 686 (Special Metals) + W, Hastelloy Alloy C2000...
Journal Articles
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
... Inconel alloy 22 is an advanced corrosion-resistant alloy with exceptional resistance to aqueous and pitting corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2004) 53 (2): Co-95.
Published: 01 February 2004
... Inconel Alloy 783 is an oxidation resistant, low expansion, nickel-cobalt-iron alloy with other additions. The alloy is a three-phase aging alloy that is of interest for close clearance control components in the aerospace arena. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1995) 44 (2): SS-580.
Published: 01 February 1995
...) or inert gas shielded arc (GTAW and GMAW) welding processes using matching filler materials. Alternatively, for welding to wrought fillings in alloys meeting ASTM B407 and B408 specifications, Inconel@ filler materials may be used. CR32W is also recommended for heat treatment furnace fiitures or any...
Journal Articles
Alloy Digest (1970) 19 (7): SS-240.
Published: 01 July 1970
... and more power is needed. Weldability: INCOLOY Alloy 802 is weldable by the shielded metal-arc process using INCaWELD* A Electrode or INCONEL* Welding Electrode 112 or by gas-shielded arc processes using INCONEL Filler Metal 82 or INCONEL Filler Metal 625. *Registered Trademark of International Nickel...
Journal Articles
Alloy Digest (1991) 40 (1): Ni-391.
Published: 01 January 1991
... are INCONEL Welding Elec- trodes 132 and 182 for shielded metal-arc welding; INCONEL Filler Metals 62 and 82 for gas tungsten-arc, gas metal-arc, and submerged-arc welding; and INCONEL Fiier Metal 62 for oxyacetylene welding. INCOFLUX 4 Submerged Arc Flux is used with the submerged-arc process. Corrosion...