Alloy Digest (1987) 36 (12): Fe-81.
Published: 01 December 1987
... INCOLOY alloy 909 is a high-strength alloy having a constant low coefficient of thermal expansion and an essentially constant rigidity up to 1200 F. The alloy is highly resistant to thermal fatigue and thermal shock. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2004) 53 (2): Co-95.
Published: 01 February 2004
... -1771 (304) 526-5100 (800) 334-4626 (304) 526-5643 (fax) United Kingdom: Special Metals Wiggin Ltd. Hereford HR4 9SL England +44-1432-382200 +44-1432-264030 (fax) ISSN: 002-614X Co-95B Fig. 1 Cyclic oxidation. Weight loss for Inconel alloys 783, 718, and Incoloy alloy 909 after 704 ºC (1300 ºF) cyclic...