1-10 of 10 Search Results for

INCOLOY ALLOY 825

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1988) 37 (6): Ni-109.
Published: 01 June 1988
... INCOLOY alloy 825 is a nickel-chromium-iron alloy with additions of molybdenum, copper, and titanium. It is resistant to chloride-ion stress-corrosion cracking, to pitting and crevice attack, and to corrosion in both oxidizing and reducing media. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2008) 57 (2): Ni-659.
Published: 01 February 2008
... Incoloy Filler Metal 65 is used for gas tungsten arc welding of Incoloy alloy 825 (See Alloy Digest Ni-109, June 1988) and other Ni-Fe-Cr-Mo-Cu alloys of similar composition. The weld metal is highly corrosion resistant, particularly in reducing chemicals such as sulfuric and phosphoric acids...
Journal Articles
Alloy Digest (1984) 33 (5): Ni-297.
Published: 01 May 1984
... 30CPF I% HzS 5% HIS 10% HzS I% HzS 5% H2S 10% H2S 4OtPF INCONEL alloy 625 8 0.0 0.3 0.1 0. I 0.4 0.2 I INCONEL alloy 7 I8 26 3.0 0.7 0. I 0.3 2.3 1.2 4 INCOLOY alloy 825 213 0. I 0.4 0. I 0. I 0.5 0.5 43 INCOLOY alloy 925 134 0. I 0.4 0. I 0. I 0.5 0.4 29 l Acidizing with HCl, 1000 psi gas phase (1% HrS...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... INCOLOY* alloy 825 :: 141 t Residue formed on surface of samples during exposure. The residue contained 81,000 ppm chlorides and I500 ppm fluorides. *INCOLOY is a registered trademark of INCO family of companies. Heat Treatment: Annealing: To anneal Carpenter 20Mo-6 stainless. heat to 2050/22OO F (I 121...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-599.
Published: 01 January 2003
... such as Inconel 601, Incoloy 800H, Incoloy 825, and equivalents; super- austenitic alloys such as UNS S31254, 254SMO, 904L, and sim- ilar alloys; cryogenic 9% Ni steels; dissimilar combinations of the above. Typical operating parameters are shown in Table 2, and fume data is shown in Table 3. Machinability...
Journal Articles
Alloy Digest (1998) 47 (2): SS-708.
Published: 01 February 1998
... Incoloy Alloy 864 is a high performance alloy developed specifically for automotive exhaust system flexible couplings and other exhaust applications. The alloy has a good combination of oxidation and corrosion resistance, with good mechanical strength, stability, and fatigue properties...
Journal Articles
Alloy Digest (2012) 61 (2): Ni-694.
Published: 01 February 2012
... the susceptibility to grain boundary. See also Fig. 1 2 and Table 2. Specification Equivalents: UNS N08825 EN 2.4858 JIS NCF 825 ASTM B424 General Characteristics: NAS 825 is a powerful corrosion-resistant alloy with a high nickel content comparable to Incoloy 825 Alloy. It provides strong resistance against both...
Journal Articles
Alloy Digest (2002) 51 (3): Ni-581.
Published: 01 March 2002
... and niobium. They are used to join UNS N06625 and Nicrofer 6020hMo of similar composition and also for other lower alloys to ensure the weld has as good or better corrosion resistance as does the base metal. Inconel and Incoloy are registered trademarks of Special Metals Corporation. Hastelloy is a registered...
Journal Articles
Alloy Digest (1998) 47 (5): Ni-542.
Published: 01 May 1998
... alloy 625, INCOLOP alloy 825. and INCO al- loy 256MO to themselves; joining the same alloys to any of the ferric, austenitic, or stainless steels; joining 9% nickel steel and various corrosion-resistant alloys, such as alloy 20. super-austenitic stainless steels, and duplex stainless steels; over- lay...
Journal Articles
Alloy Digest (1987) 36 (8): Ti-87.
Published: 01 August 1987
... Elongation (2 in.) % 15.0 21.0 20.0 22.0 23.5 Reduction of Area % 37.2 47.0 50.I 49.3 48.7 Table 3 - CORROSION RATES OF RMI BETA-C AND THREE OTHER ALLOYS Rate in Mils oer Year Test Solution and Temperature RMI Beta-C Hastelloy* Inconel** C-276 625 Incoloy** 825 1 % HCl(194 F) O-5 o-6 12-24 9-1~FeCl,11 11 f...