Alloy Digest (1978) 27 (1): SS-347.
Published: 01 January 1978
... INCOLOY Alloy 800H is a wrought austenitic alloy characterized by excellent strength and corrosion resistance at high temperatures. It has higher design strengths than the conventional stainless steels above 1100 F. It is heat treated for optimum creep and stress-to-rupture properties...
Journal Articles
Alloy Digest (1967) 16 (10): SS-201.
Published: 01 October 1967
... INCOLOY nickel-iron-chromium alloy 801 is a modification of INCOLOY alloy 800. Its nominally 1% titanium content gives it improved tensile and rupture properties. It has excellent oxidation resistance up to 1600-1700 F and can be readily formed and welded. This datasheet provides information...
Journal Articles
Alloy Digest (2005) 54 (2): SS-917.
Published: 01 February 2005
... Incoloy Alloy 832 is designed for sheathed heater applications. It is reasonably priced and contains sufficient alloying elements to develop a good surface oxide. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2006) 55 (5): SS-962.
Published: 01 May 2006
... Incoloy alloy 25-6Mo is superaustenitic, contains 6% Mo, and offers excellent corrosion resistance to neutral and acidic environments containing chlorides or other halides such as are found in air pollution control and flue gas desulfurization systems. The alloy is especially suited for service...
Journal Articles
Alloy Digest (2008) 57 (2): Ni-659.
Published: 01 February 2008
... Incoloy Filler Metal 65 is used for gas tungsten arc welding of Incoloy alloy 825 (See Alloy Digest Ni-109, June 1988) and other Ni-Fe-Cr-Mo-Cu alloys of similar composition. The weld metal is highly corrosion resistant, particularly in reducing chemicals such as sulfuric and phosphoric acids...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1056.
Published: 01 March 2010
... Incoloy alloy 25-6HN is a 6% Mo superaustenitic stainless steel. It offers an excellent combination of strength, ductility, and resistance to corrosion by a variety of media at an economical price. It is readily formed and welded. The properties of the alloy are enhanced by its content of nitrogen...
Journal Articles
Alloy Digest (1993) 42 (12): SS-559.
Published: 01 December 1993
... INCOLOY alloy 803 is a high-temperature corrosion-resistant, nickel-iron-chromium alloy, developed by Inco Alloys International for pyrolysis in high-severity ethylene furnaces, and for other petrochemical applications where high levels of oxidation-, carburization-, and/or sulfidation-resistance...
Journal Articles
Alloy Digest (1994) 43 (2): Ni-446.
Published: 01 February 1994
... INCOLOY ALLOY 908 is a nickel-iron alloy developed for applications in the advanced TOKAMAK reactor ITER. The alloy contains no cobalt, a small level of chromium to resist stress assisted grain boundary oxidation (SAGBO) and is stabilized with Cb(Nb), Ti, and Al. This datasheet provides...
Journal Articles
Alloy Digest (2014) 63 (4): Ni-666.
Published: 01 April 2014
... Incoloy Alloy 945 is a nickel-base precipitation-strengthened alloy that provides 860 MPa (125 ksi) minimum yield strength and an excellent combination of ductility and impact strength. The nickel content is sufficient to provide protection against chloride-ion stress-corrosion cracking...
Journal Articles
Alloy Digest (1957) 6 (11): SS-64.
Published: 01 November 1957
... INCOLOY-T is a nickel, chromium, iron alloy sheet primarily designed for use at moderately elevated temperatures. It possesses excellent oxidation resistance up to 1600 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1957) 6 (12): Ni-38.
Published: 01 December 1957
... INCOLOY 901 is a nickel-base alloy having creep and rupture strength at 1000 to 1400 F. It is recommended for use in aircraft and industrial gas turbine components. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (1962) 11 (9): SS-136.
Published: 01 September 1962
... INCOLOY alloy 800 is a nickel-iron-chromium alloy offering good strength along with good resistance to corrosion and oxidation at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength...
Journal Articles
Alloy Digest (1953) 2 (5): Ni-4.
Published: 01 May 1953
... INCOLOY is a heat resistant iron alloy of high percentages of nickel and chromium. It provides a high temperature alloy with excellent resistance to oxidation, good strength at elevated temperatures, and good workability and welding properties. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1970) 19 (7): SS-240.
Published: 01 July 1970
... INCOLOY ALLOY 802 is a high-carbon iron-base alloy recommended for high-temperature applications requiring excellent corrosion resistance and good mechanical properties. It is furnished in the annealed condition. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1982) 31 (9): Fe-67.
Published: 01 September 1982
... INCOLOY Alloy MA 956 is manufactured by mechanical alloying, which uniformly disperses yttrium oxide for dispersion strengthening to the alloy's melting point. The alloy combines strength at high temperatures with excellent resistance to oxidation, carburization and hot corrosion. These attributes...
Journal Articles
Alloy Digest (1986) 35 (8): SS-473.
Published: 01 August 1986
... INCOLOY Alloy DS is a wrought, austenitic nickel-chromium-iron alloy with high resistance to heat and oxidation. Its many applications include furnace parts, woven-wire conveyor belts for continuous furnaces, radiant heat tubes and gas-turbine components. This datasheet provides information...
Journal Articles
Alloy Digest (1998) 47 (2): SS-708.
Published: 01 February 1998
... Incoloy Alloy 864 is a high performance alloy developed specifically for automotive exhaust system flexible couplings and other exhaust applications. The alloy has a good combination of oxidation and corrosion resistance, with good mechanical strength, stability, and fatigue properties...
Journal Articles
Alloy Digest (2003) 52 (1): SS-871.
Published: 01 January 2003
... Incoloy alloy 27-7MO is an advanced superaustenitic stainless steel with a composition 27Ni-22Cr-7.2Mo-0.34N. In many environments this alloy performs up to the level of more highly alloyed and expensive materials such as Inconel alloy 625, 622, and C-276. This datasheet provides information...
Journal Articles
Alloy Digest (2003) 52 (8): Ni-611.
Published: 01 August 2003
... Alloy 890 provides improved properties over those of Incoloy alloys 800HT and 803 via the addition of silicon and molybdenum to optimize the performance of the alloy. Alloy 890 is typically 43% Ni, 25% Cr, 1.85 Si, 1.5% Mo, and 0.45% Nb, with the balance being principally iron. The alloy offers...
Journal Articles
Alloy Digest (2003) 52 (12): SS-895.
Published: 01 December 2003
... Incoloy alloy 028 is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. Alloy tubes can be cold worked to high strength levels for downhole service in moderately corrosive deep sour gas wells. This datasheet provides information on composition...