Publisher: Journals Gateway
Alloy Digest (2019) 68 (8): Ni-754.
Published: 01 August 2019
... Inco-Weld C-276 Welding Electrode (ENiCrMo-4) is a NiCrMo welding electrode with increased Mo, W, and reduced Nb. The alloy offers strength levels consistently exceeding the minimum requirement of the 9% nickel steels and excellent Charpy impact toughness at –196 deg C (–321 deg F). This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (1): SS-632.
Published: 01 January 1996
... INCO WELD C Electrode is a stainless-alloy electrode especially designed for shielded-metal-arc welding of a broad range of materials, including many difficult-to-weld compositions. It can be used in stainless steels, mild and medium-carbon steels,and spring steels. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (1): Ni-657.
Published: 01 January 2008
... Inco-Weld C-276 (ERNiCrMo-4) is a NiCrMo filler metal with increased molybdenum, tungsten, and reduced niobium and is suited to both gas metal arc welding (GMAW) or gas tungsten arc welding (GTAW) processes, either manually or fully automated. The alloy offers strength levels consistently...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (9): Ni-302.
Published: 01 September 1984
...) and gas metal-arc (MIG) welding of INCONEL alloy 617. For extended service at temperatures above 1700 F(925 C). it is recommended for welding INCOLOY* alloy SOOH and 802. It also is recommended for welding a number of cast alloys. *lNCONEL and INCOLOY are registered trademarks for products of the INCO...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (4): Ni-347.
Published: 01 April 1987
... INCONEL Welding Electrode 113 is used for shielded-metal-arc welding of alloy steels such as 5% nickel steel and 9% nickel steel for cryogenic applications. The weld metal has high mechanical properties, including impact values, at temperatures as low as -320 F (-196 C). Electrode 113 can...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (3): Ni-311.
Published: 01 March 1985
... INCO Alloy C-276 is a nickel-molybdenum-chromium-tungsten alloy with outstanding corrosion resistance that is maintained even in the welded condition. It also has excellent resistance to oxidizing media. It is widely used in the severest environments encountered in chemical processing, pollution...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (4): Ni-401.
Published: 01 April 1992
... corrosion. INCO, INCONEL and INCOLOY are trademarks of the INCO family of companies. Compositlon (Limiting): Physical Properties (Annealed): Nickel 24.0-26.0 Density, Ib/cu in. 0.296 Chromium 19-O-21.0 Mg/cu m 8.2 Molybdenum 6-O-7.0 Melting range, F 2410-2550 copper 0.5-1.5 C 1320-1400 Nitrogen 0.15-0.25...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (6): Ni-292.
Published: 01 June 1992
... INCO ALLOY HX is a high temperature, matrix stiffened, Ni-Cr-Fe-Mo alloy with outstanding oxidation resistance and exceptional strength at up to 2200 F (1200 C). This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (6): Ni-543.
Published: 01 June 1998
... INCO-CORED 82DH (down-hand) and 82AP (all-position) flux cored wired were developed as companion welding materials to INCONEL Filler Metal 82 and INCO-WELD A Welding Electrode. Applications include welding Inconel or Incoloy alloys to themselves or to ferritic, austenitic, or ferric/austenitic...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (12): Ni-307.
Published: 01 December 1984
... INCO-WELD B is a nickel-base alloy developed for shielded metal-arc welding of nickel steels for cryogenic applications. It is similar to INCO-WELD A Electrode (Alloy Digest Ni-305, November 1984) except that it is designed for use with alternating current to minimize magnetic arc blow. It can...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (5): Ni-403.
Published: 01 May 1992
...- loys. Hot forming should be done in the range 1750- 2100°F (955-1150°C). Weldability: Into alloy 330 is weldable by conventional processes. When shielded-metal-arc welding, use INCO-WELD* A Electrode or INCONEL* Welding Electrode 132. Gas- shielded-arc welding is done with INCONEL Filler Metal 62 or 82...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (12): SS-498.
Published: 01 December 1988
... for post-weld annealing. Use INCONEL* Welding Electrode 112 for shielded-arc weld- ing and INCONEL* FiIler Metal 625 for inert-gas shielded ttmgsten-arc welding. Corrosion Resistance: INCO alloy 020 has excellent resistance to chemical en- vironments containing sulfuric, nitric and phosphoric ac- ids...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (4): Ni-540.
Published: 01 April 1998
... Inco-Weld 725NDUR filler metal is a corrosion-resistant alloy similar to Inconel Filler Metal 625 (see Alloy Digest Ni-327, December 1985) but with higher strength and hardness. Applications include the oil exploration down-hole equipment market. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (10): Ni-341.
Published: 01 October 1986
... INCO Alloy G-3 is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to provide increased resistance to weld heat-affected zone corrosion. The alloy has exceptional stress-corrosion cracking resistance in chloride-containing environments...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (8): Ni-515.
Published: 01 August 1996
... Inco-Weld Welding Electrode 686CPT is an all-position shielded-metal-arc (SMAW) electrode with highter (CR + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (10): Ni-517.
Published: 01 October 1996
... Inco-Weld Filler Metal 686CPT is a welding product with higher (Cr + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include welding many CRA materials for corrosive service...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (7): Ni-407.
Published: 01 July 1992
... in/in F urn C Table 1 - TYPICAL MECHANICAL PROPERTIES (AS-WELDED) Tensile strength, psi 115,ooo Tensile strength, MPa 793 Elongation, % 40 Hardness, R, 100 Table 2 - TYPICAL IMPACT PROPERTIES (AS-WELDED) OF C 77 25 -320 -1% ft lb J 60 81 45 61 Table 3 - WELDABILITY Sizes and Welding Current Diameter...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (1): Ni-421.
Published: 01 January 1993
... nickel-base alloys and exhibits improved corrosion resistance over them. The aUoy could be used in reducing mineral acids and FGD equipment. @INCONEL and INCO-WELD are registered trademarks of the INCO family of companies. Chemical Composition, Wt. %: Composition (Limiting), wt % Min. Max. Carbon 0.010...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (12): Ni-327.
Published: 01 December 1985
... INCONEL Filler Metal 625 is used for gas-metal-arc and gas-tungsten-arc welding of INCONEL alloys 625 and 601 and INCOLOY alloy 800H. It is also used for surfacing of steel, for welding nickel steels, and for welding various corrosion-resistant alloys such as INCO Alloys G and 904L. It has high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (11): Ni-342.
Published: 01 November 1986
... INCONEL Filler Metal 82 is used for gas-tungsten-arc, gas-metal-arc, and submerged-arc welding of INCONEL alloys 600, 601 and 690, INCOLOY alloys 800 and 800H, and INCO alloy 330. It also is used for surfacing of steel. Dissimilar-welding applications for which the filler metal is used include...