Alloy Digest (1998) 47 (4): Ni-540.
Published: 01 April 1998
... Inco-Weld 725NDUR filler metal is a corrosion-resistant alloy similar to Inconel Filler Metal 625 (see Alloy Digest Ni-327, December 1985) but with higher strength and hardness. Applications include the oil exploration down-hole equipment market. This datasheet provides information on composition...