Alloy Digest (1998) 47 (5): Ni-542.
Published: 01 May 1998
... INCO-CORED 625DH and 625AP flux-cored wires were developed as companion welding materials to Inconel Filler Metal 625 (Alloy Digest Ni-327, December 1985) and Inconel Welding Electrode 112 (Alloy Digest Ni-313, April 1985). This datasheet provides information on composition and tensile properties...