Alloy Digest (1986) 35 (10): Ni-341.
Published: 01 October 1986
... INCO Alloy G-3 is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to provide increased resistance to weld heat-affected zone corrosion. The alloy has exceptional stress-corrosion cracking resistance in chloride-containing environments...
Journal Articles
Alloy Digest (1985) 34 (12): Ni-327.
Published: 01 December 1985
... INCONEL Filler Metal 625 is used for gas-metal-arc and gas-tungsten-arc welding of INCONEL alloys 625 and 601 and INCOLOY alloy 800H. It is also used for surfacing of steel, for welding nickel steels, and for welding various corrosion-resistant alloys such as INCO Alloys G and 904L. It has high...
Journal Articles
Alloy Digest (1992) 41 (5): Ni-403.
Published: 01 May 1992
... INCO ALLOY 330 is a nickel/iron/chromium austenitic alloy, not hardenable by heat treatment. It is a solid solution strengthened high-temperature alloy. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1996) 45 (1): SS-632.
Published: 01 January 1996
... composition hardness INCO-WELD C joinability tensile properties weldability welding electrodes UNS W31310 may - DIGEST - INCO-WELD C DATA ON WORLD WIDE METALS AND ALLOYS Filing Code ss-632 a Stainless Steels - January 1996 @G?py@t 19%. ASM Inremstimel. All rights res~oetashownererypica.nottote...
Journal Articles
Alloy Digest (1995) 44 (10): Ni-488.
Published: 01 October 1995
... NILOMAG ALLOY 77 is a 77 Ni soft magnetic alloy with a high level of initial permeability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Ni-488. Producer or source: Inco Alloys...
Journal Articles
Alloy Digest (1996) 45 (8): Ni-515.
Published: 01 August 1996
... Inco-Weld Welding Electrode 686CPT is an all-position shielded-metal-arc (SMAW) electrode with highter (CR + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include...
Journal Articles
Alloy Digest (1985) 34 (3): Ni-311.
Published: 01 March 1985
... INCO Alloy C-276 is a nickel-molybdenum-chromium-tungsten alloy with outstanding corrosion resistance that is maintained even in the welded condition. It also has excellent resistance to oxidizing media. It is widely used in the severest environments encountered in chemical processing, pollution...
Journal Articles
Alloy Digest (1993) 42 (1): Ni-421.
Published: 01 January 1993
..., physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance, and corrosion resistance. Filing Code: Ni-421. Producer or source: Inco Alloys International Inc. Producer or Source: Inco Alloys International Inc. Copyright © ASM...
Journal Articles
Alloy Digest (1996) 45 (10): Ni-517.
Published: 01 October 1996
... Inco-Weld Filler Metal 686CPT is a welding product with higher (Cr + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include welding many CRA materials for corrosive service...
Journal Articles
Alloy Digest (1987) 36 (3): SS-482.
Published: 01 March 1987
...: Inco Alloys International Inc.. Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties elasticity fracture toughness heat treatability high-temperature alloys INCOLOY ALLOY 800HT joinability machinability physical...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-410.
Published: 01 August 1992
.... This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: Ni-410. Producer or source: Inco Alloys International Inc...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-313.
Published: 01 April 1985
... INCONEL Welding Electrode 112 is a nickel-base alloy that is used for welding INCONEL alloys 625 and 601 and INCOLOY alloy 800H. It is also used for surfacing steel and various corrosion-resistant alloys such as HUNTINGTON alloys G and 9041. It is useful for joining dissimilar metals involving...
Journal Articles
Alloy Digest (1989) 38 (5): Al-296.
Published: 01 May 1989
... on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-296. Producer or source: Inco Alloys International Inc.. Producer or Source...
Journal Articles
Alloy Digest (1993) 42 (12): SS-559.
Published: 01 December 1993
... INCOLOY alloy 803 is a high-temperature corrosion-resistant, nickel-iron-chromium alloy, developed by Inco Alloys International for pyrolysis in high-severity ethylene furnaces, and for other petrochemical applications where high levels of oxidation-, carburization-, and/or sulfidation-resistance...
Journal Articles
Alloy Digest (1990) 39 (5): Ni-382.
Published: 01 May 1990
... on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-382. Producer or source: Inco Alloys International Inc.. Producer or Source: Inco Alloys International Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion...
Journal Articles
Alloy Digest (1994) 43 (11): Ni-471.
Published: 01 November 1994
..., INCONEL alloy 718SPF sheet meets the suength and ductility requirements of AMS 55%G. as annealed plus aged. Table 3 compares the annealed pmperties of INCONEL alloy 718SPF with that of SPF material with teductions in gauge of 13%. 19% and 33%. Note that. under these conditions. the alloy exceeds...
Journal Articles
Alloy Digest (2002) 51 (1): Ni-577.
Published: 01 January 2002
... 0.001 Copper 0.001 Lead 0.001 Nickel bal Physical Properties: Density, kg/m3 (lb/in.3 ) 7700 (0.278) General Characteristics: Incomag Alloy 3LC is a nickel-base alloy containing 4.0 5.0% Mg and about 0.025% C. This foundry additive alloy was devel- oped by Inco for the production of ductile iron...
Journal Articles
Alloy Digest (1987) 36 (9): Ni-351.
Published: 01 September 1987
... properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-351. Producer or source: Inco Alloys International Inc.. Copyright © ASM International® 1996 1996 ASM...
Journal Articles
Alloy Digest (1998) 47 (2): SS-708.
Published: 01 February 1998
... at corresponding Celsius and Fahrenheit lcmpmmm. rcspeaiuly. Table 2 Intergranular Corrosion Test Results ASTMAW-E ASlMAXlX -+ -+ Alby I+rmm&d u4)oFllb Ash -Tm 864 No craCki Noaacking 10 55 321 No Crachll~ No cmckiog 26 64 316-G 48 s-521 Table 3 Stress Corrosion Cracking Test Results in Boiling 45% MgC12 U-Bend...
Journal Articles
Alloy Digest (1970) 19 (4): Ni-152.
Published: 01 April 1970
... Electrolytic Pickling Water Sulfuric Acid (660 Bd) lgal 1000 cc % Dt 95 cc Sodium Fluoride . 3 & Temperature Room Time As Required Container: Rubber-Lined Steel Tank Corrosion Resistance: 25 g Room As Required INCONEL alloy 601 has outstanding resistance to oxidation and scaling at high temperatures. Figure 3...