Alloy Digest (1992) 41 (5): Ni-403.
Published: 01 May 1992
... INCO ALLOY 330 is a nickel/iron/chromium austenitic alloy, not hardenable by heat treatment. It is a solid solution strengthened high-temperature alloy. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1986) 35 (11): Ni-342.
Published: 01 November 1986
... INCONEL Filler Metal 82 is used for gas-tungsten-arc, gas-metal-arc, and submerged-arc welding of INCONEL alloys 600, 601 and 690, INCOLOY alloys 800 and 800H, and INCO alloy 330. It also is used for surfacing of steel. Dissimilar-welding applications for which the filler metal is used include...
Journal Articles
Alloy Digest (1985) 34 (10): Ni-323.
Published: 01 October 1985
... IONCONEL Welding Electrode 132 is used for shielded-metal-arc welding of INCONEL alloys 600 and 601 and INCO alloy 330. Electrode 132 has good dissimilar-welding capability. Examples are joining INCONEL and INCOLOY alloys to carbon steels, stainless steels, nickel and MONEL alloys. It also is used...
Journal Articles
Alloy Digest (1998) 47 (6): Ni-543.
Published: 01 June 1998
... and 8OOHT; and INCO alloy 330 to them- selves and to each other. (See Alloy Digest Ni-176. Ni-152. Ni-266. SS-136. SS-347. SS-482, and Ni-403.) Joining the same alloys to ferric and austenitic steels, or du- plex stainless and stainless steels Overlay cladding of carbon steels and heat treatable low alloy...
Journal Articles
Alloy Digest (1992) 41 (4): Ni-401.
Published: 01 April 1992
... INCO Alloy 25-6 MO is a highly alloyed austenitic nickel/iron alloy that is especially resistant to non-oxidizing acids such as sulfuric and phosphoric. It is also well suited to handle high-chloride environments and to combat microbially influenced corrosion. (See updated alloy Incoloy Alloy 25...
Journal Articles
Alloy Digest (1990) 39 (5): Ni-382.
Published: 01 May 1990
... on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-382. Producer or source: Inco Alloys International Inc.. Producer or Source: Inco Alloys International Inc. Copyright ┬ę ASM International┬« 1996 1996 ASM International chemical composition corrosion...
Journal Articles
Alloy Digest (1982) 31 (9): Fe-67.
Published: 01 September 1982
... includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-67. Producer or source: Huntington Alloy Products Division, An INCO Company. Producer or Source: Huntington Alloy Products Division, An INCO Company...
Journal Articles
Alloy Digest (2006) 55 (5): SS-962.
Published: 01 May 2006
... in high chloride environments such as brackish water, seawater, caustic chloride, and pulp mill bleach systems. This alloy is similar to Inco Alloy 25-6Mo (See Alloy Digest Ni-401, April 1992) and supersedes it. This datasheet provides information on composition, physical properties, hardness, elasticity...