Skip Nav Destination
Close Modal
Search Results for
IN-102
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 500
Search Results for IN-102
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1973) 22 (12): Ni-198.
Published: 01 December 1973
... PYROMET 102 is a nonmagnetic, nickel-chromium base alloy which is solid solution strengthened by the refractory metals niobium, tungsten and molybdenum. It possesses excellent corrosion properties, strength, ductility, toughness and structural stability. It is used as tubing and piping for steam...
Abstract
View articletitled, PYROMET <span class="search-highlight">102</span>: Solid Solution Strengthened Alloy
View
PDF
for article titled, PYROMET <span class="search-highlight">102</span>: Solid Solution Strengthened Alloy
PYROMET 102 is a nonmagnetic, nickel-chromium base alloy which is solid solution strengthened by the refractory metals niobium, tungsten and molybdenum. It possesses excellent corrosion properties, strength, ductility, toughness and structural stability. It is used as tubing and piping for steam and gas turbines, rocket engines, heat shields, furnace hardware, chemical plant hardware and in sea water environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-198. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1969) 18 (1): W-12.
Published: 01 January 1969
... Sylvania WN-102 is a tungsten-base alloy combining high density with high strength in both compression and tension. It is recommended for radioactive shielding, counterweights, electrical contacts for high currents, gyroscopes, flywheels and governors. This datasheet provides information...
Abstract
View articletitled, SYLVANIA WN-<span class="search-highlight">102</span>: Heavy Metal
View
PDF
for article titled, SYLVANIA WN-<span class="search-highlight">102</span>: Heavy Metal
Sylvania WN-102 is a tungsten-base alloy combining high density with high strength in both compression and tension. It is recommended for radioactive shielding, counterweights, electrical contacts for high currents, gyroscopes, flywheels and governors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on forming, machining, and joining. Filing Code: W-12. Producer or source: Sylvania Electric Products Inc..
Journal Articles
Alloy Digest (1969) 18 (9): Ni-147.
Published: 01 September 1969
... IN-102 is a nickel-chromium-iron alloy designed for long service at temperatures up to 1300 F. It combines high strength and high ductility at the elevated temperatures with a high degree of structural stability. It is used for aerospace, power and steam turbine components. This datasheet provides...
Abstract
View articletitled, IN-<span class="search-highlight">102</span>: High Temperature Alloy
View
PDF
for article titled, IN-<span class="search-highlight">102</span>: High Temperature Alloy
IN-102 is a nickel-chromium-iron alloy designed for long service at temperatures up to 1300 F. It combines high strength and high ductility at the elevated temperatures with a high degree of structural stability. It is used for aerospace, power and steam turbine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-147. Producer or source: International Nickel Company Inc..
Journal Articles
Alloy Digest (1979) 28 (3): Cu-368.
Published: 01 March 1979
... Copper No. 102 is a wrought oxygen-free high-conductivity copper. Its trade designation is OF (Oxygen Free) copper. It can be fabricated by all the conventional methods and is used widely for bus bars, bus conductors and other electrical conductors. This datasheet provides information...
Abstract
View articletitled, COPPER ALLOY No. <span class="search-highlight">102</span>: Oxygen Free Copper
View
PDF
for article titled, COPPER ALLOY No. <span class="search-highlight">102</span>: Oxygen Free Copper
Copper No. 102 is a wrought oxygen-free high-conductivity copper. Its trade designation is OF (Oxygen Free) copper. It can be fabricated by all the conventional methods and is used widely for bus bars, bus conductors and other electrical conductors. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-368. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (2016) 65 (2): SA-741.
Published: 01 February 2016
... PERFORM 700 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 700 in the title refers to the minimum yield strength in MPa (102 ksi). The USA equivalent is Perform 102. This datasheet provides information on composition...
Abstract
View articletitled, PERFORM 700: Structural Steel for Cold Forming
View
PDF
for article titled, PERFORM 700: Structural Steel for Cold Forming
PERFORM 700 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 700 in the title refers to the minimum yield strength in MPa (102 ksi). The USA equivalent is Perform 102. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming and joining. Filing Code: SA-741. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Alloy Digest (2017) 66 (1): Cu-856.
Published: 01 January 2017
... Alloy KHP 102 (UNS C19010) is a high performance copper alloy with additions for strength while maintaining high conductivity. KHP 102 belongs to the group of CuNiSi alloys and is particularly suitable for use in electrical and electronic products. This datasheet provides information...
Abstract
View articletitled, KEMPER KHP102: Copper/Nickel/Silicon Alloy
View
PDF
for article titled, KEMPER KHP102: Copper/Nickel/Silicon Alloy
Alloy KHP 102 (UNS C19010) is a high performance copper alloy with additions for strength while maintaining high conductivity. KHP 102 belongs to the group of CuNiSi alloys and is particularly suitable for use in electrical and electronic products. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: Cu-856. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Alloy Digest (1992) 41 (12): Ti-102.
Published: 01 December 1992
... on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on heat treating. Filing Code: Ti-102. Producer or source: Timet. Producer or Source: Timet Copyright © ASM International® 1996 1996 ASM International...
Abstract
View articletitled, TIMETAL 62S: Low Cost, Multipurpose Titanium Alloy
View
PDF
for article titled, TIMETAL 62S: Low Cost, Multipurpose Titanium Alloy
TIMETAL 62S, because iron is used for the beta stabilizer in lieu of more expensive elements, has a lower formulation cost than most titanium alloys, yet the properties and processing characteristics of Ti-6A1-2Fe-0. 1Si are equivalent to or better than those of the workhorses of the titanium industry, including Ti-6A1-4V. The combination of reasonable cost and excellent mechanical properties make TIMETAL 62S a practical substitute for other engineering materials in numerous industrial applications that require low weight and high corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on heat treating. Filing Code: Ti-102. Producer or source: Timet.
Journal Articles
Alloy Digest (1993) 42 (11): Fe-102.
Published: 01 November 1993
..., and surface treatment. Filing Code: FE-102. Producer or source: Carpenter. Producer or Source: Carpenter Copyright © ASM International® 1996 1996 ASM International Carpenter Glass Sealing 42 ceramic-to-metal seals chemical composition elasticity hardness heat treatability joinability...
Abstract
View articletitled, CARPENTER GLASS SEALING 42: Controlled Expansion Alloy
View
PDF
for article titled, CARPENTER GLASS SEALING 42: Controlled Expansion Alloy
CARPENTER GLASS SEALING 42 has wide-ranging applications in glass-to-metal and ceramic-to-metal sealing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: FE-102. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1996) 45 (11): Co-102.
Published: 01 November 1996
... provides information on composition, physical properties, and elasticity as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CO-102. Producer or source: VDM Technologies Corporation...
Abstract
View articletitled, CONICRO 4023 W: High-Temperature, Heat-Resistant, Cobalt-Base Alloy
View
PDF
for article titled, CONICRO 4023 W: High-Temperature, Heat-Resistant, Cobalt-Base Alloy
Conicro 4023 W is a high-temperature, heat-resistant, cobalt-base alloy with equal contents of nickel and chromium, a high tungsten content, and a controlled lanthanum addition. The alloy has excellent mechanincal properties and scaling resistance to 1150 deg C (2100 deg F). This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CO-102. Producer or source: VDM Technologies Corporation.
Journal Articles
Alloy Digest (1965) 14 (6): Ni-102.
Published: 01 June 1965
..., hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-102. Producer or source: Latrobe Steel Company. Producer or Source: Latrobe...
Abstract
View articletitled, LESCALLOY 718 VAC-ARC: Age-Hardenable High-Temperature Alloy
View
PDF
for article titled, LESCALLOY 718 VAC-ARC: Age-Hardenable High-Temperature Alloy
LESCALLOY 718 VacArc is a precipitation hardening nickel-base super alloy designed for service at elevated temperatures up to 1300 F where high strength coupled with good ductility and corrosion resistance are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-102. Producer or source: Latrobe Steel Company.
Journal Articles
Alloy Digest (2019) 68 (11): SA-855.
Published: 01 November 2019
... Aldur® 700 steels (minimum yield strength of 700 MPa, or 102 ksi, for thicknesses up to 50 mm, or 2 in.) are a part of a family of water-quenched, high-strength, fine-grained steels that have excellent toughness at low temperatures. This datasheet provides information on composition, physical...
Abstract
View articletitled, ALDUR 700Q, QL, QL1: Structural Steel
View
PDF
for article titled, ALDUR 700Q, QL, QL1: Structural Steel
Aldur® 700 steels (minimum yield strength of 700 MPa, or 102 ksi, for thicknesses up to 50 mm, or 2 in.) are a part of a family of water-quenched, high-strength, fine-grained steels that have excellent toughness at low temperatures. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: SA-855. Producer or source: Voestalpine Grobblech GmbH.
Journal Articles
Alloy Digest (2023) 72 (2): CI-102.
Published: 01 February 2023
... than the impact and elongation properties. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on casting and heat treating. Filing Code: CI-102. Producer or source: ACO Eurobar GmbH...
Abstract
View articletitled, ACO EUROBAR EN-GJS-350-22C (5.3122): Continuous Cast Spheroidal Graphite Cast Iron
View
PDF
for article titled, ACO EUROBAR EN-GJS-350-22C (5.3122): Continuous Cast Spheroidal Graphite Cast Iron
ACO Eurobar EN-GJS-350-22C is a ferritic spheroidal graphite cast iron that is produced by the continuous casting process. It has a minimum tensile strength of 350 MPa (51 ksi) and a minimum elongation of 22%. It is specifically designed for applications where tensile strength is less important than the impact and elongation properties. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on casting and heat treating. Filing Code: CI-102. Producer or source: ACO Eurobar GmbH.
Journal Articles
Alloy Digest (1976) 25 (4): Zn-27.
Published: 01 April 1976
... MICROZINC Alloy 100 is a zinc-lead-cadmium alloy having good ductility with adequate strength, good resistance to corrosion, and a low coefficient of sliding friction. It is solderable and non-magnetic. Processing differences give three commercial products or classes designated= 101, 102 and 103...
Abstract
View articletitled, MICROZINC ALLOY 100: Ductile, Atmospheric Corrosion Resistant Alloy
View
PDF
for article titled, MICROZINC ALLOY 100: Ductile, Atmospheric Corrosion Resistant Alloy
MICROZINC Alloy 100 is a zinc-lead-cadmium alloy having good ductility with adequate strength, good resistance to corrosion, and a low coefficient of sliding friction. It is solderable and non-magnetic. Processing differences give three commercial products or classes designated= 101, 102 and 103. This alloy does not stain other materials. Its many uses include jewelry, coins and battery cans. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zn-27. Producer or source: Ball Corporation, Metal and Chemical Division.
Journal Articles
Alloy Digest (2007) 56 (5): SA-567.
Published: 01 May 2007
... Weldox 700 is a general structural steel with a minimum yield strength of 700 MPa (102 ksi). This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA...
Abstract
View articletitled, WELDOX 700: High-Strength Structural Steel Plate
View
PDF
for article titled, WELDOX 700: High-Strength Structural Steel Plate
Weldox 700 is a general structural steel with a minimum yield strength of 700 MPa (102 ksi). This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-567. Producer or source: SSAB Weldox.
Journal Articles
Alloy Digest (1960) 9 (3): SS-102.
Published: 01 March 1960
.... It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-102. Producer or source: Cyclops Corporation. Producer or Source: Cyclops Corporation Copyright © ASM International® 1996 1996 ASM...
Abstract
View articletitled, UNILOY 1430MV: Heat and Corrosion Resisting Steel
View
PDF
for article titled, UNILOY 1430MV: Heat and Corrosion Resisting Steel
UNILOY 1430MV is a high-chromium, molybdenum heat and corrosion resisting steel used for highly stressed parts involving service temperatures up to 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-102. Producer or source: Cyclops Corporation.
Journal Articles
Alloy Digest (1960) 9 (8): SA-102.
Published: 01 August 1960
... performance as well as forming, heat treating, machining, and joining. Filing Code: SA-102. Producer or source: Babcock & Wilcox Company. Producer or Source: Babcock & Wilcox Company Copyright © ASM International® 1996 1996 ASM International chemical composition elasticity fracture...
Abstract
View articletitled, NICLOY 3 1/2: Low Temperature Service Steel
View
PDF
for article titled, NICLOY 3 1/2: Low Temperature Service Steel
NICLOY 3 1/2 is a low carbon, nickel ferritic steel recommended for low temperature service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-102. Producer or source: Babcock & Wilcox Company.
Journal Articles
Alloy Digest (1961) 10 (2): TS-102.
Published: 01 February 1961
... as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-102. Producer or source: Uddeholm (Canada) Ltd. Producer or Source: Uddeholm (Canada) Ltd Copyright © ASM International® 1996 1996 ASM International chemical composition...
Abstract
View articletitled, UHB ORVAR: Hot Work Tool Steel, Type H13
View
PDF
for article titled, UHB ORVAR: Hot Work Tool Steel, Type H13
UHB-ORVAR is a die casting die steel and a general hot work steel. It is air-hardening, non-deforming, and has high resistance to heat checking and erosive action. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-102. Producer or source: Uddeholm (Canada) Ltd.
Journal Articles
Alloy Digest (1961) 10 (4): Al-102.
Published: 01 April 1961
..., and bearing strength as well as fracture toughness and fatigue. It also includes information on as well as forming, heat treating, machining, and joining. Filing Code: Al-102. Producer or source: James Booth & Company Ltd. Producer or Source: James Booth & Company Ltd Copyright © ASM...
Abstract
View articletitled, DURALUMIN-K: Heat Treatable, Wrought Aluminum Alloy
View
PDF
for article titled, DURALUMIN-K: Heat Treatable, Wrought Aluminum Alloy
Duralumin-K is a high strength, wrought aluminum alloy recommended for highly stressed applications. It responds to the precipitation-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fracture toughness and fatigue. It also includes information on as well as forming, heat treating, machining, and joining. Filing Code: Al-102. Producer or source: James Booth & Company Ltd.
Journal Articles
Alloy Digest (1961) 10 (6): Cu-102.
Published: 01 June 1961
... Cu-66, August 1958). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: Cu-102. Producer or source: The International...
Abstract
View articletitled, NI-VEE TYPE B: Constructional Bronze
View
PDF
for article titled, NI-VEE TYPE B: Constructional Bronze
NI-VEE TYPE B is a precipitation hardening nickel bronze alloy suitable for constructional castings. This alloy provides the advantage of maximum strength in contact with steel or similar hard and strong coostruction material. It has improved machinability compared with Ni-Vee Type A (Alloy Digest Cu-66, August 1958). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: Cu-102. Producer or source: The International Nickel Company Inc..
Journal Articles
Alloy Digest (1984) 33 (7): CS-102.
Published: 01 July 1984
... information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-102. Producer or source: Carbon steel mills. Producer or Source: Carbon steel mills Copyright © ASM International® 1996 1996 ASM International AISI 1146 axles ball joints bolts...
Abstract
View articletitled, AISI 1146: Free Cutting Carbon Steel
View
PDF
for article titled, AISI 1146: Free Cutting Carbon Steel
AISI 1146 is a resulfurized carbon steel containing nominally 0.85% manganese and a range of 0.08-0.13% sulfur to make it free machining. It has relatively low hardenability. Its ductility and toughness are fairly good in the longitudinal direction but are low in the transverse direction. It is recommended highly for high-production automatic machine products. Among its many uses are axles and shafts, screws, spindles, ball joints, gears, bolts and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-102. Producer or source: Carbon steel mills.
1