Alloy Digest (1962) 11 (11): Al-120.
Published: 01 November 1962
... IMPALCO 770 is a heat treatable, high strength aluminum alloy available in bar form for machining applications. It is recommended for highly stressed structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...