Alloy Digest (1962) 11 (4): Fe-20.
Published: 01 April 1962
... Hyflux Alnico V-7 is a high energy permanent magnet capable of achieving typical energy values of 7 million BH max. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code...