Alloy Digest (1971) 20 (10): Ni-5.
Published: 01 October 1971
... Carpenter HYMU 80 is an unoriented 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability and maximum permeability with minimum hysteresis loss at low magnetic field strengths. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1989) 38 (10): Ni-375.
Published: 01 October 1989
... CARPENTER HyMu 80 alloy is an unoriented soft magnetic alloy with extremely high initial permeability as well as maximum permeability with minimum hysteresis loss. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1997) 46 (12): Ni-133.
Published: 01 December 1997
... trademark of Westinghouse El&c Cotporation Carpenter and HyMu 80 aUoy are trademarksofczarpenter T&logy Corp.- Chemical Composition, wL%: Physical Properties: tkRSilY.kehdm31 speifice 8746 (03 la) 8.14 31.4Cl8.1) 1450 (2642) 0.6 (MO) CnriemrpasmrrTm 4600 cDefiiciandTupto538T 0.00 11(0.ooo6) @EPF~~IO lOWoF...