Alloy Digest (1962) 11 (8): SA-133.
Published: 01 August 1962
... Hy-Ten B Temper No. 2 is a low-chromium medium-carbon steel combining strength, toughness and wear resistance. It is recommended for gears, rolls, shafts and other machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1960) 9 (9): SA-103.
Published: 01 September 1960
... HY-TEN B TEMPER No. 3-X is a strong, tough alloy steel of high hardenability recommended for heavy duty applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1970) 19 (1): SA-248.
Published: 01 January 1970
... HY-TEN B Temper No. 3X-40 is a medium-carbon alloy steel having free-cutting characteristics. It is recommended for machine tools, mining and road building equipment, gears, crankshafts, bolts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1979) 28 (4): SA-358.
Published: 01 April 1979
... - AVERAGE NUMBER OF INCLUSIONS IN THE WORST FIELD OBSERVED FOR THE DIFFERENT TYPES OF INCLUSIONS (Based on ASTM E45 JK-Chart - Method A - for a 20-inch diameter Cabot ESR HY 140 ingot) Type A Type B The C Type D Diameter (Sulfides) (Alumina) (Silicates) (Globular Oxides) Condition in. Thin Heavy Thin Heavy...
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
... by conventional processes. Cold forming may be carried out in the quenched and tempered condition and typical bend radii are 2T for 180 degrees. Cold forming will result in some loss in impact strength and large plastic strains (in excess of about ten percent) should be avoided. Weldability: Ingersoll-Rand ESR HY...
Journal Articles
Alloy Digest (1959) 8 (8): SA-88.
Published: 01 August 1959
.... A- Pseudo carburized, quenched or cooled slowly in box, reheated to 1450 F., quenched in oil, tempered. As quenched 112000 75000 27 207 70 200 110000 75000 it 207 70 300 110000 75000 33; 62 207 75 400 110000 75000 30 63 207 500 110000 75000 67 207 ;i 600 110000 75000 22: 70 207 98 B -Pseudo carburized...