Alloy Digest (2005) 54 (4): TS-616.
Published: 01 April 2005
... HOTVAR is a high-performance molybdenum-vanadium alloyed hot-work tool steel. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating, machining, and joining. Filing Code: TS-616. Producer or source: Böhler Uddeholm...