Alloy Digest (1968) 17 (7): Cu-189.
Published: 01 July 1968
... Hitenso-1622 is a copper-cadmium alloy characterized by high strength, abrasion resistance and relatively high electrical conductivity. (Formerly known as Hitenso BB-961). It is recommended for electrical equipment, trolley wire, low temperature transmission lines and relays. This datasheet...