Journal Articles
Alloy Digest (2002) 51 (10): Fe-124.
Published: 01 October 2002
... Hiperco Alloy 15 is a development in soft magnetic alloys that combines the properties of high saturation, magnetization, high electrical resistivity, and lower cobalt content. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1988) 37 (2): Co-83.
Published: 01 February 1988
... CARPENTER HIPERCO 50 is a magnetic soft alloy used primarily as magnetic core in electrical equipment requiring high permeability at very high magnetic flux densities. These magnetic characteristics permit weight reduction, reduction of copper turns and insulation in the end product in comparison...
Journal Articles
Alloy Digest (1964) 13 (7): Fe-26.
Published: 01 July 1964
... Hiperco 27 is an iron-cobalt type of soft magnetic material recommended for use in motors, generators, transformers and relays and at temperatures above 950 F. It is used for high flux levels. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1970) 19 (1): Fe-41.
Published: 01 January 1970
... Hiperco 35 is an iron-cobalt type of soft magnetic material recommended for use in motors, generators, transformers and relays at temperature above 950 F. It yields the highest known saturation value of 24,500 gausses. This datasheet provides information on composition, physical properties...