Skip Nav Destination
Close Modal
Search Results for
Heat Treatment
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 5523 Search Results for
Heat Treatment
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (3): SS-71.
Published: 01 March 1958
... CIRCLE L17 is an age-hardening type of stainless steel having the desirable mechanical properties of the hardenable chromium type corrosion resisting steel combined with workability and corrosion resistance approaching 18-8 type stainless steel. It is hardenable by heat treatment to Rockwell C40...
Abstract
View article
PDF
CIRCLE L17 is an age-hardening type of stainless steel having the desirable mechanical properties of the hardenable chromium type corrosion resisting steel combined with workability and corrosion resistance approaching 18-8 type stainless steel. It is hardenable by heat treatment to Rockwell C40-45. Cracking, distortion, decarburization, scaling and similar problems encountered after machining are virtually eliminated due to the low heat treatment temperature required for hardening. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: SS-71. Producer or source: Lebanon Steel Foundry.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (5): SS-3.
Published: 01 May 1989
... ARMCO 17-7 PH is a precipitation-hardening stainless steel that provides high strength and hardness, excellent fatigue strength, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition, then hardens to high strength levels by simple heat...
Abstract
View article
PDF
ARMCO 17-7 PH is a precipitation-hardening stainless steel that provides high strength and hardness, excellent fatigue strength, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition, then hardens to high strength levels by simple heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-3. Producer or source: Baltimore Specialty Steels Corporation. Originally published December 1952, revised May 1989.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (3): Ni-163.
Published: 01 March 1971
... PYROMET X-750 is a precipitation-hardenable nickel-base alloy that is highly resistant to chemical corrosion and oxidation and has excellent stress-rupture and creep properties at temperatures up to 1500 F after suitable heat treatment. This datasheet provides information on composition, physical...
Abstract
View article
PDF
PYROMET X-750 is a precipitation-hardenable nickel-base alloy that is highly resistant to chemical corrosion and oxidation and has excellent stress-rupture and creep properties at temperatures up to 1500 F after suitable heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-163. Producer or source: Carpenter Technology Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): Cu-724.
Published: 01 May 2013
... ToughMet 2 is a high performance, wrought, heat treatable, lead-free strip Cu-Ni alloy that imparts superior mechanical performance and high thermal stability to plain bearing applications. Parts are easily formed and they can be machined either before or after heat treatment. ToughMet alloys...
Abstract
View article
PDF
ToughMet 2 is a high performance, wrought, heat treatable, lead-free strip Cu-Ni alloy that imparts superior mechanical performance and high thermal stability to plain bearing applications. Parts are easily formed and they can be machined either before or after heat treatment. ToughMet alloys are a line of spinodal hardened Cu-Ni anti-galling alloys for bearings capable of performing with a variety of shafting materials and lubricants. The alloys combine a high lubricity with wear resistance in these severe loading conditions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming and machining. Filing Code: Cu-724. Producer or source: Materion Brush Performance Alloys. Originally published September 2004, revised May 2013.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (3): Al-474.
Published: 01 March 2021
... properties. It offers good strength in the as-cast condition and is often used that way. However, it is possible to increase strength considerably by heat treatment. In applications that experience high temperatures, as in engine components, it is common to employ a T5, T7, or O treatment. These treatments...
Abstract
View article
PDF
Rio Tinto 319.2 is a heat-treatable, Al-Si-Cu casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. Alloy 319.0 exhibits very good castability and pressure tightness, moderate strength, and good high-temperature properties. It offers good strength in the as-cast condition and is often used that way. However, it is possible to increase strength considerably by heat treatment. In applications that experience high temperatures, as in engine components, it is common to employ a T5, T7, or O treatment. These treatments tend to stabilize the casting and reduced dimensional changes in the component caused by high temperatures in service. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-474. Producer or source: Rio Tinto Limited.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (4): Al-102.
Published: 01 April 1961
... Duralumin-K is a high strength, wrought aluminum alloy recommended for highly stressed applications. It responds to the precipitation-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear...
Abstract
View article
PDF
Duralumin-K is a high strength, wrought aluminum alloy recommended for highly stressed applications. It responds to the precipitation-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fracture toughness and fatigue. It also includes information on as well as forming, heat treating, machining, and joining. Filing Code: Al-102. Producer or source: James Booth & Company Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Ni-767.
Published: 01 February 2021
.... Special Precautions Exposure of ATI 80 A to sulfurous atmospheres at elevated temperatures must be avoided. Also, the parts must be care- fully cleaned to completely remove all sulfur-based machin- ing oils or lubricants prior to welding or heat treatment. Comparable Grades Fig. 3 Modulus of elasticity...
Abstract
View article
PDF
ATI 80 A is a wrought, precipitation-hardenable, Ni-Cr-Ti-Al alloy that is generally used for high strength applications up to 760 °C (1400 °F), but may also be used at temperatures up to 845 °C (1550 °F) for short duration service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ni-767. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (11): Co-107.
Published: 01 November 1999
... 752 °F) 10.0 (5.6) 25 600 °C (77 1112 °F) 10.5 (5.8) 25 800 °C (77 1472 °F) 11.3 (6.3) Coercive force, HC, from 16,000 A/m (200 Oe), A/m (Oe) Laminations or tape cores made from strip, annealed at 871 °C (1600 °F) 32 (0.4) Standard heat treatment of bar, annealed at 871 °C (1600 °F) 150 (1.9) Duplex...
Abstract
View article
PDF
Hiperco 50A is an iron-cobalt-vanadium soft magnetic alloy possessing high magnetic saturation, high direct current (dc) maximum permeability, low dc coercive force, and low alternating current (ac) core loss. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on heat treating. Filing Code: CO-107. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (7): Fe-78.
Published: 01 July 1987
... Nonmagnetic PROPERTIES Table 1 - TYPICAL TENSILE PROPERTIES Test Tensile Yield Strength Elongation Reduction Temperature Strength (0.2% Offset) (2 in.150.8 mm) of Area OF ( C) psi (MPa) psi (MPa) % % Heat Treatment A (See Heat Treatment Section) 70 (21) 172000 (1180) 120000 (820) 14 23 1000 (538) 151000 (1040...
Abstract
View article
PDF
PYROMET CTX-3 is a high-strength precipitation-hardenable low-expansion superalloy. It exhibits a low coefficient of thermal expansion over a broad temperature range combined with high strength. The alloy possesses high hot hardness and good resistance to thermal fatigue. It is brazable, weldable and can be plated with chromium. CTX-3 uses comprise compressor and exhaust casings, seals and other components for gas turbine engines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-78. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (5): TS-813.
Published: 01 May 2021
... forging, the parts should be air cooled to linear thermal 25 93 °C room temperature and then annealed. Following the anneal, expansion(a) 10 6/K (75 200 °F) 9.99 the forgings should be normalized in order to restore prop- (10 6/°F) (5.55) erties to the dead zone. 25 204 °C (75 400 °F) 10.58 Heat Treatment...
Abstract
View article
PDF
CarTech AerMet-for-Tooling is a low-carbon, cobalt-nickel-chromium-molybdenum, alloy tool steel that exhibits high strength and high hardness together with exceptional ductility and toughness. This alloy is designed for components that require a hardness of about 53–55 HRC along with very high toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-813. Producer or source: Carpenter Technology Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (6): Fe-148.
Published: 01 June 2009
... of cryogenic, room temperature, and elevate temperature properties are available for producer. See also Table 1 and Fig. 1 3. Heat Treatment: Decarburization. AerMet 340 is subject to decarburization during hardening. Heat treatment should take place in a neutral atmosphere furnace, salt bath, or vacuum...
Abstract
View article
PDF
Carpenter AerMet 340 Alloy possesses high hardness and strength while exhibiting exceptional toughness and ductility, and can be considered for a variety of automotive, racing, aerospace, and defense applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, and machining. Filing Code: FE-148. Producer or source: Carpenter Specialty Alloys.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (6): TS-541.
Published: 01 June 1996
... expansion. le. in/i . F 5.6 Thermal conductivity (400 to 1 lOOoF). (Btu/ft . h . F) 17 Before modifying the above procedures or applying any surface treatments, consult the producer. Weldability: Heat Treatment: Crucible Marlok is supplied in the solution-annealed condition having a hardness of 28 to 32...
Abstract
View article
PDF
Crucible Marlok is a maraging ultrahigh-strength fully martensitic die steel with a relating low-precipitation treatment. It is used in long-run or high-finish aluminum casting operations. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-541. Producer or source: Crucible Service Centers.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (3): Ni-688.
Published: 01 March 2011
... NAS 600 is a nickel alloy with 14-17 chromium and has excellent oxidation resistance. The alloy is used extensively in heat treatment furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...
Abstract
View article
PDF
NAS 600 is a nickel alloy with 14-17 chromium and has excellent oxidation resistance. The alloy is used extensively in heat treatment furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-688. Producer or source: Nippon Yakin Kogyo Company Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (4): Al-463.
Published: 01 April 2020
...: J.G. Kaufman and E.L. Rooy, Aluminum Alloy Castings: Properties, Processes, and Applications, ASM International, 2004 Mechanical Properties See Tables 1, 2, and 3. Heat Treatment See Table 4. Comparable Grades Ingot Casting Rio Tinto Ltd. 242.2 242.0 ISO EN JIS ASTM B179:2018 242.2 ASTM...
Abstract
View article
PDF
Rio Tinto Alloy 242.2 is a heat-treatable, aluminum-copper-magnesium-nickel casting alloy. It is available in the form of ingots to be remelted for the manufacture of sand and permanent mold castings. Alloy 242.0 is used extensively for applications requiring high strength and hardness at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, machining, and joining. Filing Code: Al-463. Producer or source: Rio Tinto Limited.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (6): Ni-638.
Published: 01 June 2006
... C (1300 deg F). The strength can be increased by heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni...
Abstract
View article
PDF
HPM X-750 is a precipitation-hardenable nickel-chromium alloy that is well suited for a wide range of corrosive and oxidizing environments where strength must be maintained to elevated temperatures. The alloy composition provides a product that performs well at elevated temperatures up to 700 deg C (1300 deg F). The strength can be increased by heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-638. Producer or source: Hamilton Precision Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (9): SA-308.
Published: 01 September 1974
... 40000 2050 20 69000 2050 30 78000 2050 50 88000 2100 30 88000 Heat Treatment: Microstructure: IN-86 I P/M steel is used in the as-sintered condition and requires no further heat treatment. This eliminates the problems (such as distortion, cracking. surface finish and degreasingj normally associated...
Abstract
View article
PDF
IN-861 is a mixed elemental powder metallurgy steel designed for use in the as-sintered condition. It achieves its good mechanical properties by hardening during normal cooling in most commercial sintering furnaces. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on heat treating, machining, and powder metal forms. Filing Code: SA-308. Producer or source: International Nickel Company Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (1): Fe-46.
Published: 01 January 1971
..., and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: Fe-46. Producer or source: Cyclops Corporation. Producer or Source: Cyclops Corporation Copyright © ASM...
Abstract
View article
PDF
UNISPAN LR35 offers the lowest coefficient of thermal expansion of any alloy now available. It is a low residual modification of UNISPAN 36 for fully achieving the demanding operational level of precision equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: Fe-46. Producer or source: Cyclops Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (6): Cu-217.
Published: 01 June 1970
... Yield Strength Rockwell Electrical Heat Strength Limit 0.002% 0.2% Offset Elongation Hardness Conductivity Ternpert Treatment* Psi offset, psi psi Q in 2 in. B or C Scale Q I.A.C.S. A - 60- 85,000 15- 22.000 20- 30,000 35-60 B45-85 17-19 Vi H or H 85-130.000 35- 65.000 75-105,000 10-30 888-103 15-17...
Abstract
View article
PDF
BRUSH alloy M25 is a free-machining beryllium-copper alloy having good response to age-hardening for high strength, hardness, fatigue and corrosion resistance. It is recommended for screw machine products, gears, shafts, hardware, fasteners, connectors, electronic and electrical components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-217. Producer or source: Brush Beryllium Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (3): Ni-380.
Published: 01 March 1990
... temperature. Fig. 2 -Typical stress-rupture life. Copyright © ASM International® 1996DOI: 10.31399/asm.ad.ni0380 Heat Treatment: ALLVAC 500 ZB heat treatment consists of 4 steps: Solutiontreatment*:soakfor2hoursat2150°F(11770C) air cool. (Hardness will be Rc23-28). Preliminary aging: 1975oF (1079 C) for 4...
Abstract
View article
PDF
ALLVAC 500 ZB is an austenitic precipitation hardening alloy which develops outstanding tensile, fatigue and stress-rupture properties. It is suited to longtime service requirements up to 1800 F (982 C). It is produced by vacuum induction melting plus vacuum arc remelting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-380. Producer or source: Allvac Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (3): Ni-188.
Published: 01 March 1973
... of elasticity, psi 22x106 Curie temperature, Oc 500 PROPERTIES Table 1 - MAGNETIC PROPERTIES - Strip (Hydrogen annealed at 2 150oF and control cooled, as recommended under Heat Treatment) Saturation flux density, gausses 15500-15800 Squareness, minimum 0.94 Coercive force (d.c oersteds 0.10-0.15 Table 2...
Abstract
View article
PDF
BLENDALLOY 25-5000 is a nickel-iron alloy with a rectangular hysteresis loop and low coercive force. It is a powder metallurgy product and this helps to provide it with uniform and consistent magnetic properties, exceptional purity and cleanliness, precise chemcial composition and guaranteed reproducibility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-188. Producer or source: Spang Industries Inc..