Alloy Digest (1961) 10 (3): Ni-64.
Published: 01 March 1961
... Haynes No. 713C is a nickel-base, vacuum melted, vacuum-cast alloy with excellent high-strength characteristics through 1800 F. It combines extraordinarily high strength with good ductility. It is a precipitation-hardening investment-cast alloy. This datasheet provides information on composition...