1-8 of 8 Search Results for

Haynes alloy no. 56

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1961) 10 (11): SS-123.
Published: 01 November 1961
... HAYNES alloy No. 56 is a high temperature alloy having excellent strength and oxidation resistance in the 1200 to 1900 F temperature range. (Pat. No. 2,513,470) This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1985) 34 (8): Ni-320.
Published: 01 August 1985
... HAYNES Alloy No. 230 is essentially a cobalt-free, nickel-base alloy with outstanding high-temperature strength, oxidation resistance and thermal stability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (1971) 20 (1): Co-62.
Published: 01 January 1971
... HAYNES Alloy No. 188 is a cobalt-base alloy which has excellent high-temperature strength, outstanding oxidation resistance, and good post-aging ductility. It is recommended for aircraft engine components. (U.S. Pat. 3,418,111 This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1971) 20 (5): Ni-164.
Published: 01 May 1971
... is readily machinable by conven- tional methods. Tungsten carbide tipped tools are suggested. It also can be machined with HAYNES 98M2 alloy or HAYNES Star J-Metal tools with excellent results, but at lower surface speeds (HAYNES is a registered trademark). High-speed steel tools also can be used. Because...
Journal Articles
Alloy Digest (1993) 42 (8): Ni-440.
Published: 01 August 1993
...-Resistant Alloy) HASTELLOY@ alloy C-276 is a solid solution, nickel-molybdenum-chromium alloy, with outstanding resistance to localized corrosion and to both oxidizing and reducing media. (See Alloy Digest Ni-164 for b&e metal.) - @HASTELLOY is a trademark of Haynes International, Inc. Chemical Composition...
Journal Articles
Alloy Digest (1999) 48 (5): Ni-552.
Published: 01 May 1999
... Hastelloy B-3 alloy welding products are used to promote similar corrosion resistance to Hastelloy B-3 (Alloy Digest Ni-461, August 1994) and B-2 (Alloy Digest Ni-249, September 1997) base metals, for the dissimilar welding of Hastelloy B-3 and B-2 to nickel or iron-base corrosion resistant alloys...
Journal Articles
Alloy Digest (2002) 51 (10): Ni-592.
Published: 01 October 2002
..., and it is used to join high-molybdenum-containing corrosion-resistant alloys to themselves and each other by tungsten inert gas (TIG) welding. Hastelloy and C22 are trademarks of Haynes International, Inc. Inconel is a registered trademark of Special Metals Corporation. Table 1 Fume Data Fume composition, wt...