Alloy Digest (1961) 10 (12): Co-5.
Published: 01 December 1961
... HAYNES# Alloy No. 25 is a wrought, high temperature, cobalt-base alloy that has exceptional mechanical properties at temperatures up to 1800 deg. F. in the fully annealed condition without subsequent aging. It is easy to fabricate because it has excellent ductility at room temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
... HAYNES Alloy No. 36 is a cobalt-base alloy having excellent strength at temperatures up to 1800 deg. F. It is the cast modification of wrought HAYNES Alloy No. 25 and has been used successfully in jet engine blading and nozzle vanes. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... Alloy No. 6B Mill aNlNlcd 8.2 HAYNES STELLlTE Alloy No. 6K Mi8atlmdcd 13.3 HAYNES 8TELLll-E Alloy No. 25 Mill aNNaled (16000F. 1 ht) 53.0 AN1090 steel WV** + 9000F. 4 min 37.2 AlSl Type 316 Stainlas Steel As-tecclvcd sheet 81.4 ALSl Type 304 St&less Steel As-received sheet 102.1 Rockwell Hardness C-38 C...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
... welding followed by furnace cooling. Standard weld joints are recommended. HAYNES alloy No. 25 or HASTELLOY alloy W filler metals are recommended for joining the cobalt-base alloys to softer materials such as carbon steel or stainless steel, while the harder cobalt-base filer metals are recommended...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (11): Ni-395.
Published: 01 November 1991
... (25) 5.4 ( 37) 3.5 ( 24) 1.9 (13) 3.6 ( 25) 1.7( 12) 0.8 (5.5) 2.0 ( 14) 0.8 ( 5.5) - - Heat Treatment: HAYNES HR-120 alloy is a solid solution strengthened ahoy. It is not hardenable by heat treatment. Workability: HAYNESHR-12Oalloymaybereadilyhotorcoldworked. Welding: HAYNES FIR-120 alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (7): Co-22.
Published: 01 July 1960
... HAYNES STELLITE 98M2 Alloy is a cobalt-base alloy having higher compressive strength and higher hardness than all the other cobalt-base alloys at room temperature and in the red heat range. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (3): Ni-64.
Published: 01 March 1961
... Haynes No. 713C is a nickel-base, vacuum melted, vacuum-cast alloy with excellent high-strength characteristics through 1800 F. It combines extraordinarily high strength with good ductility. It is a precipitation-hardening investment-cast alloy. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (1): Co-62.
Published: 01 January 1971
... HAYNES Alloy No. 188 is a cobalt-base alloy which has excellent high-temperature strength, outstanding oxidation resistance, and good post-aging ductility. It is recommended for aircraft engine components. (U.S. Pat. 3,418,111 This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... + 10% cold reduced 1.5 c44 1.00 x 10-3 Ditto Ma + 18.5% cold reduced 7.8 c-47 1.00 x 10-3 HAYNES STELLITE Alloy No. 6K Mill annealed 13.3 C46 0.946 x 10-3 HAYNES STELLITE Alloy NO. 25 Mill annealed ( 1600°F, 1 hr) 53.0 C-24 2.00 x IO-3 AlSl 1090 Steel WQ + 9OoOF. 4 min 37.2 c-55 8.00 x 10-3 AlSl Type...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (6): SA-165.
Published: 01 June 1964
... HAYNES Alloy No. 90 is a high-chromium high-carbon iron-base alloy recommended for handling extreme conditions of wear, abrasion, and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (7): Ni-557.
Published: 01 July 1999
... Haynes alloy 75 is an 80 nickel-20 chromium alloy with both good oxidation resistance and good mechanical properties at high temperatures. It is amenable to all forms of fabrication and welding. A typical application for sheet metal is fabrications in gas turbine engines. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (9): Ni-755.
Published: 01 September 2019
... Haynes HR-233 has excellent oxidation resistance and improved fabricability and weldability. The alloy can be used to 1150 deg C (2100 deg F). This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (2): Ni-558.
Published: 01 February 2000
... Haynes 230-W Filler Wire is a specially formulated welding filler metal designed for the fabrication of Haynes 230 alloy (see Alloy Digest Ni-320, August 1985). This datasheet provides information on composition, physical properties, elasticity, and bend strength. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (5): Ni-759.
Published: 01 May 2020
... Haynes 233 is a new nickel-cobalt-chromium-molybdenum-aluminum alloy that offers excellent oxidation resistance up to 1150 °C (2100 °F) or higher, coupled with superior creep strength—a combination of properties never before achieved in a readily fabricable alloy. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (10): Ni-763.
Published: 01 October 2020
... Haynes HR-224 is a wrought Ni-27.5Fe-20Cr-3.8Al alloy with excellent oxidation resistance and with improved fabricability and weldability as compared to Haynes 214. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1962) 11 (5): Co-31.
Published: 01 May 1962
... HAYNES STELLITE Star J-Metal is a cobalt-base alloy recommended for handling extreme conditions of wear, abrasion and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (1): Ni-399.
Published: 01 January 1992
... Haynes 242 Alloy is age hardenable by long-range-Ordering. It has good oxidation resistance and maintains good strength up to about 1300 F (705 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (11): Co-84.
Published: 01 November 1988
... HAYNES ALLOY No. 150 is a cobalt-base alloy with excellent thermal shock resistance. It has a higher melting point than other cobalt-and nickel-base high-temperature alloys and resists high-temperature corrosion in air and air-sulfur dioxide atmospheres. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (9): Ni-464.
Published: 01 September 1994
.... Producer or source: Haynes International Inc. Producer or Source: Haynes International Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys HASTELLOY D-205 alloy joinability tensile properties HASTFI I Oy@ D-2()5TM ALLOY :i%z...