Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
... Haynes Stellite No. 4 is a cobalt-base cast alloy recommended for handling severe conditions of abrasion, heat and corrosion. It is especially recommended to resist the severe abrasive and corrosive action of manganese dioxide, carbon particles, and ammonium and zinc chlorides in the battery mix...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... + 10% cold reduced 1.5 c44 1.00 x 10-3 Ditto Ma + 18.5% cold reduced 7.8 c-47 1.00 x 10-3 HAYNES STELLITE Alloy No. 6K Mill annealed 13.3 C46 0.946 x 10-3 HAYNES STELLITE Alloy NO. 25 Mill annealed ( 1600°F, 1 hr) 53.0 C-24 2.00 x IO-3 AlSl 1090 Steel WQ + 9OoOF. 4 min 37.2 c-55 8.00 x 10-3 AlSl Type...
Journal Articles
Alloy Digest (1960) 9 (7): Co-22.
Published: 01 July 1960
.... It also has a higher compressive strength. In terms of actual rates of metal removal, Haynes Stellite 98M2 alloy is one of the most efficient 5 - 15 5- 10 o-5 o-7 o-5 o-5 3-7 4-7 3-5 3-7 4-7 3-5 o-45 o-45 o-45 5-15 5-20 5 - 10 l/64 - l/4 l/64 - l/4 l/64 - l/4 metal-cutting tools. This alloy has red...
Journal Articles
Alloy Digest (1958) 7 (5): Co-13.
Published: 01 May 1958
... HAYNES STELLITE No. 19 is a cobalt-base cutting tool alloy having high resistance to severe shock and excellent red-hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1980) 29 (5): Ni-263.
Published: 01 May 1980
... No. I 2 (2.7) 4 (5.4) STELLITE alloy No. 6 9 (12.2) 17 (23) HAYNES alloy No. 40 l(l.4) 2 (2.7) RUBBER WHEEL U WEAR TEST SAND PARTICLES and METAL WEAR Fig. 1 - Abrasive wear test unit (dry sand). DOI: 10.31399/asm.ad.ni0263 Copyright © ASM International® 1996 FORCE t ALLOY WEAR TEST SPECIMEN...
Journal Articles
Alloy Digest (1962) 11 (5): Co-31.
Published: 01 May 1962
... HAYNES STELLITE Star J-Metal is a cobalt-base alloy recommended for handling extreme conditions of wear, abrasion and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1962) 11 (2): Co-30.
Published: 01 February 1962
... HAYNES STELLITE Alloy No. 12 is a cobalt-base alloy having high heat and corrosion resistance with excellent wear and abrasion resistance. It will withstand moderate shock and impact. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... HAYNES STELLITE Alloy No. 6B is a cobalt-base alloy that is highly resistant to most types of wear. It has long service life even under constant erosive conditions, and it exhibits high resistance to seizure and galling even without lubricants. Its corrosion resistance is good in a wide variety...
Journal Articles
Alloy Digest (1982) 31 (3): Ni-274.
Published: 01 March 1982
...-tungsten arc [TIC] weld deposits*) Average CharBy Impact WOY (No Notch) ft-lb (J-I HAYNES alloy No. N-6 10 (13.6) STELLITE alloy No. 6 17 (23) HAYNFS alloy No. 716 9 (12.2) HAYNES alloy No. 711 2 (2.7) STELLITE aIloy No. 1 4 (5.4) DELORO alloy No. 60 2 (2.7) *Undiluted. -. k&u m <At room tem&aturej 8000...
Journal Articles
Alloy Digest (1962) 11 (5): Co-14.
Published: 01 May 1962
... Haynes Stellite Alloy No. 6 is a cobalt-base high-carbon alloy having high heat and thermal shock resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1960) 9 (11): Co-8.
Published: 01 November 1960
... HAYNES STELLITE Alloy No. 31 is a cobalt-base, high-temperature alloy having high tensile and creep properties in precision castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes...
Journal Articles
Alloy Digest (1953) 2 (5): Co-1.
Published: 01 May 1953
... HAYNES STELLITE ALLOY No. 21 is a cobalt-base alloy containing chromium and molybdenum. It is resistant to oxidizing and reducing atmospheres up to 2100 F. It has excellent strength at elevated temperatures that is maintained through aging characteristics occurring in the temperature range of 1300...
Journal Articles
Alloy Digest (1964) 13 (6): SA-165.
Published: 01 June 1964
... HAYNES Alloy No. 90 is a high-chromium high-carbon iron-base alloy recommended for handling extreme conditions of wear, abrasion, and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1961) 10 (3): Ni-64.
Published: 01 March 1961
..., physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as machining. Filing Code: Ni-64. Producer or source: Haynes Stellite Company. Producer or Source: Haynes Stellite...
Journal Articles
Alloy Digest (1964) 13 (9): Co-40.
Published: 01 September 1964
... Haynes Alloy No. 152 is a cobalt-base, high-temperature casting alloy. It is designed for gas-turbine components requiring high strength properties in the 1000 to 2000 F temperature range. This datasheet provides information on composition, physical properties, and tensile properties as well...
Journal Articles
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
... properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-17. Producer or source: Haynes Stellite Company. Producer or Source...
Journal Articles
Alloy Digest (1963) 12 (11): Cb-6.
Published: 01 November 1963
... Carbide Corporation, Stellite Division Copyright © ASM International® 1996 1996 ASM International bearing strength chemical composition creep properties elasticity hardness Haynes alloy Cb-752 heat treatability high-temperature alloys joinability machinability nuclear reactors...
Journal Articles
Alloy Digest (1971) 20 (1): Co-62.
Published: 01 January 1971
... or Source: Stellite Division, Cabot Corporation Copyright © ASM International® 1996 1996 ASM International aircraft engine components chemical composition corrosion-resistant alloys creep properties ductility elasticity fracture toughness HAYNES alloy no. 188 heat treatability high...
Journal Articles
Alloy Digest (1961) 10 (12): Co-5.
Published: 01 December 1961
... Code: Co-5. Producer or source: Haynes Stellite Company. Originally published September 1953, revised December 1961. Producer or Source: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties...