Alloy Digest (1962) 11 (5): Co-14.
Published: 01 May 1962
... Haynes Stellite Alloy No. 6 is a cobalt-base high-carbon alloy having high heat and thermal shock resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1982) 31 (3): Ni-274.
Published: 01 March 1982
... STELLlTE* alloy No. 6 has been used successfully. *HAYNES, STELLITE and DELORO are @&red trademarks of Cabot Corporation. [The properties listed herein are based on laboratory tests by the manufachuer and should not be used for specification or final design. The secondary units (metric) are those of the SI...
Journal Articles
Alloy Digest (1963) 12 (11): Cb-6.
Published: 01 November 1963
... Carbide Corporation, Stellite Division Copyright © ASM International® 1996 1996 ASM International bearing strength chemical composition creep properties elasticity hardness Haynes alloy Cb-752 heat treatability high-temperature alloys joinability machinability nuclear reactors...
Journal Articles
Alloy Digest (1962) 11 (2): Co-30.
Published: 01 February 1962
... to temperatures as high as 20000F. Its resistance to oxidation, corrosion and erosion is excellent. It is harder and more abrasion resistant than Haynes Stellite Alloy No. 6, but will withstand only moderate shock or impact. For applications involving corrosion plus abrasion, the use of &is alloy is particularly...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... HAYNES STELLITE alloy No. 6K is a cobalt-base alloy with outstanding resistance to most types of wear. Its wear resistance is a built-in characteristic and not the result of heat-treatment, plating, nitriding, or other methods used to produce a superficial hardness on metal parts. Among its many...
Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... HAYNES STELLITE Alloy No. 6B is a cobalt-base alloy that is highly resistant to most types of wear. It has long service life even under constant erosive conditions, and it exhibits high resistance to seizure and galling even without lubricants. Its corrosion resistance is good in a wide variety...
Journal Articles
Alloy Digest (1980) 29 (5): Ni-263.
Published: 01 May 1980
... 475 440 380 260 TIC 620 510 465 390 230 STELLITE alloy No. 6 OA 450 350 295 265 I80 lx Et :z 27s 260 185 HAYNES alloy No. 40 E 440 245 II0 585 555 440 250 I15 *OA = Oxyacetylene. TIC = GasTungsten Arc. -Tested in vacuum fumaa of hot hardness unit. 159O.g load with 136-d~. sapphire indenter. tMermnd...
Journal Articles
Alloy Digest (1960) 9 (11): Co-8.
Published: 01 November 1960
... HAYNES STELLITE Alloy No. 31 is a cobalt-base, high-temperature alloy having high tensile and creep properties in precision castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes...
Journal Articles
Alloy Digest (1960) 9 (7): Co-22.
Published: 01 July 1960
... HAYNES STELLITE 98M2 Alloy is a cobalt-base alloy having higher compressive strength and higher hardness than all the other cobalt-base alloys at room temperature and in the red heat range. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
... Haynes Stellite No. 4 is a cobalt-base cast alloy recommended for handling severe conditions of abrasion, heat and corrosion. It is especially recommended to resist the severe abrasive and corrosive action of manganese dioxide, carbon particles, and ammonium and zinc chlorides in the battery mix...
Journal Articles
Alloy Digest (1962) 11 (5): Co-31.
Published: 01 May 1962
... HAYNES STELLITE Star J-Metal is a cobalt-base alloy recommended for handling extreme conditions of wear, abrasion and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
...: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties elasticity fracture toughness Haynes alloy no. 36 heat treatability high-temperature alloys jet engine components joinability...
Journal Articles
Alloy Digest (1961) 10 (3): Ni-64.
Published: 01 March 1961
... alloy. l Tbe term Haynes is a registered trademark of Union Carbide Corporation. Composition: Physical Constants: Carbon 0.08-0.20 Specific gravity Manpnese 0.25 max. Density, lb./cu.in. g;;ez 0.015 max. Thermal coef. expansion/of x lo-6 (loo-2000F) 0.50 max. (loo-16OOOF) Chromium 12.0-14.0 Molybdenum...
Journal Articles
Alloy Digest (1964) 13 (6): SA-165.
Published: 01 June 1964
... HAYNES Alloy No. 90 is a high-chromium high-carbon iron-base alloy recommended for handling extreme conditions of wear, abrasion, and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1971) 20 (1): Co-62.
Published: 01 January 1971
... or Source: Stellite Division, Cabot Corporation Copyright © ASM International® 1996 1996 ASM International aircraft engine components chemical composition corrosion-resistant alloys creep properties ductility elasticity fracture toughness HAYNES alloy no. 188 heat treatability high...
Journal Articles
Alloy Digest (1996) 45 (9): Co-99.
Published: 01 September 1996
... solidification of a hard and corrosion-resistant intenneMic compound. known as Laves phase. Tribaloyisaregisterednadema& of Stoody Deloro Stellite, Inc. Hastelloy is a trademark of Haynes International. Inc.. and Ninatic is a t&emarkofArmcoSteel. Chemical Composition, wt Wad) carbon cm8 ChKUtliUttl 18 Molybdenum...
Journal Articles
Alloy Digest (1961) 10 (12): Co-5.
Published: 01 December 1961
... Code: Co-5. Producer or source: Haynes Stellite Company. Originally published September 1953, revised December 1961. Producer or Source: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties...
Journal Articles
Alloy Digest (1957) 6 (8): Ni-36.
Published: 01 August 1957
..., and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-36. Producer or source: Haynes Stellite Company. Producer or Source: Haynes Stellite Company Copyright...
Journal Articles
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements...