Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... HAYNES STELLITE alloy No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... 14.2 7.9 14.5 9 ii:: 15.5 8.6 Fig. 1 - Abrasive wear test unit (Dry sand). Table 3 - AVERAGE ABRASIVE WEAR DATA ON ALLOY No. 6K AND FIVE OTHER ALLOYS* Volume Loss Rockwell Wear MOY Condition mm3 Hardness Coefficient** -- HAYNES STELLITE Alloy No. 68 Mill annealed (Ma) 8.2 C-38 0.471 x 10-3 Ditto Ma...
Journal Articles
Alloy Digest (1960) 9 (7): Co-22.
Published: 01 July 1960
.... It also has a higher compressive strength. In terms of actual rates of metal removal, Haynes Stellite 98M2 alloy is one of the most efficient 5 - 15 5- 10 o-5 o-7 o-5 o-5 3-7 4-7 3-5 3-7 4-7 3-5 o-45 o-45 o-45 5-15 5-20 5 - 10 l/64 - l/4 l/64 - l/4 l/64 - l/4 metal-cutting tools. This alloy has red...
Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... HAYNES STELLITE Alloy No. 6B is a cobalt-base alloy that is highly resistant to most types of wear. It has long service life even under constant erosive conditions, and it exhibits high resistance to seizure and galling even without lubricants. Its corrosion resistance is good in a wide variety...
Journal Articles
Alloy Digest (1958) 7 (5): Co-13.
Published: 01 May 1958
... HAYNES STELLITE No. 19 is a cobalt-base cutting tool alloy having high resistance to severe shock and excellent red-hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1980) 29 (5): Ni-263.
Published: 01 May 1980
... 475 440 380 260 TIC 620 510 465 390 230 STELLITE alloy No. 6 OA 450 350 295 265 I80 lx Et :z 27s 260 185 HAYNES alloy No. 40 E 440 245 II0 585 555 440 250 I15 *OA = Oxyacetylene. TIC = GasTungsten Arc. -Tested in vacuum fumaa of hot hardness unit. 159O.g load with 136-d~. sapphire indenter. tMermnd...
Journal Articles
Alloy Digest (1962) 11 (5): Co-31.
Published: 01 May 1962
... HAYNES STELLITE Star J-Metal is a cobalt-base alloy recommended for handling extreme conditions of wear, abrasion and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1953) 2 (5): Co-1.
Published: 01 May 1953
... HAYNES STELLITE ALLOY No. 21 is a cobalt-base alloy containing chromium and molybdenum. It is resistant to oxidizing and reducing atmospheres up to 2100 F. It has excellent strength at elevated temperatures that is maintained through aging characteristics occurring in the temperature range of 1300...
Journal Articles
Alloy Digest (1962) 11 (5): Co-14.
Published: 01 May 1962
... Haynes Stellite Alloy No. 6 is a cobalt-base high-carbon alloy having high heat and thermal shock resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1960) 9 (11): Co-8.
Published: 01 November 1960
... HAYNES STELLITE Alloy No. 31 is a cobalt-base, high-temperature alloy having high tensile and creep properties in precision castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes...
Journal Articles
Alloy Digest (1982) 31 (3): Ni-274.
Published: 01 March 1982
... STELLlTE* alloy No. 6 has been used successfully. *HAYNES, STELLITE and DELORO are @&red trademarks of Cabot Corporation. [The properties listed herein are based on laboratory tests by the manufachuer and should not be used for specification or final design. The secondary units (metric) are those of the SI...
Journal Articles
Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
... Haynes Stellite No. 4 is a cobalt-base cast alloy recommended for handling severe conditions of abrasion, heat and corrosion. It is especially recommended to resist the severe abrasive and corrosive action of manganese dioxide, carbon particles, and ammonium and zinc chlorides in the battery mix...
Journal Articles
Alloy Digest (1961) 10 (3): Ni-64.
Published: 01 March 1961
... Haynes No. 713C is a nickel-base, vacuum melted, vacuum-cast alloy with excellent high-strength characteristics through 1800 F. It combines extraordinarily high strength with good ductility. It is a precipitation-hardening investment-cast alloy. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1964) 13 (9): Co-40.
Published: 01 September 1964
... Haynes Alloy No. 152 is a cobalt-base, high-temperature casting alloy. It is designed for gas-turbine components requiring high strength properties in the 1000 to 2000 F temperature range. This datasheet provides information on composition, physical properties, and tensile properties as well...
Journal Articles
Alloy Digest (1964) 13 (6): SA-165.
Published: 01 June 1964
... HAYNES Alloy No. 90 is a high-chromium high-carbon iron-base alloy recommended for handling extreme conditions of wear, abrasion, and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1959) 8 (3): Co-17.
Published: 01 March 1959
...: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties elasticity fracture toughness Haynes alloy no. 36 heat treatability high-temperature alloys jet engine components joinability...
Journal Articles
Alloy Digest (1963) 12 (11): Cb-6.
Published: 01 November 1963
... Carbide Corporation, Stellite Division Copyright © ASM International® 1996 1996 ASM International bearing strength chemical composition creep properties elasticity hardness Haynes alloy Cb-752 heat treatability high-temperature alloys joinability machinability nuclear reactors...
Journal Articles
Alloy Digest (1961) 10 (12): Co-5.
Published: 01 December 1961
... Code: Co-5. Producer or source: Haynes Stellite Company. Originally published September 1953, revised December 1961. Producer or Source: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties...
Journal Articles
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements...
Journal Articles
Alloy Digest (1956) 5 (11): Ni-29.
Published: 01 November 1956
... as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-29. Producer or source: Haynes Stellite Company. Producer or Source: Haynes Stellite Company Copyright © ASM International® 1996 1996 ASM...