Alloy Digest (2020) 69 (10): Ni-763.
Published: 01 October 2020
... Haynes HR-224 is a wrought Ni-27.5Fe-20Cr-3.8Al alloy with excellent oxidation resistance and with improved fabricability and weldability as compared to Haynes 214. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2017) 66 (3): Ni-727.
Published: 01 March 2017
... Haynes HR-224 has excellent oxidation resistance and improved fabricability and weldability compared to Haynes 214 alloy. This datasheet provides information on composition and tensile properties. It also includes information on high temperature performance as well as forming. Filing Code: Ni-727...
Journal Articles
Alloy Digest (1963) 12 (11): Cb-6.
Published: 01 November 1963
... ZircYooium 2.5 Carbon 40 pm Oxygen 60 pm Nitrogen < 100 ppm Hydrogen 6 pm Columbium Remainder Specific gravity Dhnsity, lb/cu;in. Specific heat, Btu/lb/oF at 320F at 1000.22000F Thermal coef. ex 8 nsion/oF x lo-6 8- 2000F 68-10000F 68-16000F 68-22000F Thermal conductivity, Btu/ft2/in/hr/oF at 500oF...
Journal Articles
Alloy Digest (1993) 42 (4): Ni-425.
Published: 01 April 1993
... 932 1112 Specific heat, Btu/lbPF 0.089 0.093 0.097 0.101 0.103 0.106 0.109 Thermalconductivity, Btu/ft2~m./hr/ F 77 85 93 102 111 120 130 Electrical resistivity, microhm-in. 54.1 54.3 54.5 54.6 54.8 55.6 57.6 ThermaI diffusivity. in.%ec. 0.005 0.005 0.006 0.006 0.006 0.007 0.007 Table 3 - TYPICAL WELD...