Alloy Digest (2004) 53 (6): Ni-621.
Published: 01 June 2004
... Hastelloy C-22HS has, like the other C-type alloys, excellent corrosion resistance, but it also exhibits high strength, nearly double the other alloys in the family. (See updated datasheet Alloy Digest Ni-742, March 2018.) This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (3): Ni-742.
Published: 01 March 2018
... Hastelloy C-22HS is a Ni-Cr-Mo alloy that exhibits an exceptional combination of mechanical properties and corrosion resistance in the cold-worked (CW) condition. This is an updated revision of Alloy Digest Ni-621, June 2004. This datasheet provides information on composition, physical properties...